| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | STN EN ISO 294-4 |
|
Plastcom PLASTAMID® 66 GF 15 T 15 TS PA66 reinforced with glass fibers and mineral filler, heat stabilized
Black PA66 for injection molding, reinforced with 15% glass fiber and 15% mineral filler, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of elect..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | Euronil |
|
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
-
0.0080
cm/cm @Thickness 3.20 mm |
0.0060
-
0.0080
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East)
Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated |
|
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound
(Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
cm/cm @Temperature 80.0 °C |
0.0060
in/in @Temperature 176 °F |
60x60x2 mm; ISO 294-4 |
|
Gromax BFG45-B100N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | |
|
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4, 2577 |
|
Lanxess Pocan® C 3230 XF 000000 PBT + PC, 30% Glass Fiber
PBT+PC, 30% glass fibers, injection molding, improved flowability, low tendency to warp, improved surface finish
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0075 cm/cm | 0.0060 - 0.0075 in/in | |
|
LATI Latiohm 87/28-07 CNT PC
Semiconductive/dissipative product based on Polycarbonate (PC). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
|
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
-
0.0080
cm/cm @Time 86400 sec |
0.0060
-
0.0080
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP STAT-KON DD0009E PC
LNP* STAT-KON* DD0009E is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant, Easy Molding.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
cm/cm @Thickness 3.20 mm |
0.0060
in/in @Thickness 0.126 in |
ASTM D955 |
|
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber
Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low ..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
-
0.010
cm/cm @Thickness 3.20 mm |
0.0060
-
0.010
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.0090 cm/cm | 0.0060 - 0.0090 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
-
0.0080
cm/cm @Time 86400 sec |
0.0060
-
0.0080
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF002H PC
LNP THERMOCOMP* DF002H is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added feature includes: Healthcare.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
-
0.0080
cm/cm @Time 86400 sec |
0.0060
-
0.0080
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES
LNP* THERMOCOMP* JF006E is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
cm/cm @Thickness 3.20 mm |
0.0060
in/in @Thickness 0.126 in |
ASTM D955 |
|
Samsung Cheil Industries Starex® HR-0370F ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 - 0.010 cm/cm | 0.0060 - 0.010 in/in | DIS 294-4 |
|
Wellman Wellamid® FRGF1850-BK1 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant
All information provided by Wellman Engineered Resins.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
cm/cm @Thickness 3.00 mm |
0.0060
in/in @Thickness 0.118 in |
|
|
Toyobo VYLOPET® CA5310 PC/PBT Polymer Alloy, High Rigidity, Impact Resistant
Applications: Lamp partsHome electric appliance partsFeatures: Fine appearanceHigh rigidityImpact resistantInformation provided by Toyobo.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated |
|
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy
Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66
(Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long t..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® HTN 51G35HSL NC010 Polyphthalamide (PPA)
(Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL NC010 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40
Product description: Grivory HT1V-4 FWA black 9225 is a 40 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50
Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
|
Barlog Plastics KEBAFLEX SG 55 A.01 TPE-S, Shore A55, natural
TPE-SInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
|
Barlog Plastics KEBAFLEX SG 60 A.01 black TPE-S, Shore A60, black
TPE-SInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | |
|
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0060
-
0.0080
cm/cm @Time 86400 sec |
0.0060
-
0.0080
in/in @Time 24.0 hour |
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp JX89569 PES (Asia Pacific)
LNP* THERMOCOMP* JX89569 is a compound based on Polyethersulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)
(Unverified Data**)
45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ASTM D955 |
|
LG Chemical LUPOL GP-2201F General Purpose Polypropylene, 20% Glass Fiber Reinforced, Flame Retardant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
|
|||