Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0070 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Asia Pacific)
High flow PC+ABS.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS
Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0040 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Geloy FXTW26SK ASA
Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® HPS6 PC (Asia Pacific)
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Time 86400 sec
0.0050 - 0.0070 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC
LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.18 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.125 in
5&quot; x 0.5&quot; x 0.125&quot; bars; ASTM D955
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK) &nbsp;(Unverified Data**)
AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+PS
LNP* Lubricomp* Noryl_SPN422L compound is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Ultem 1010RF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM 2212EPR PEI (Asia Pacific)
20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising.
Linear Mold Shrinkage, Transverse 0.0040 - 0.0070 cm/cm
<br>@Time 86400 sec
0.0040 - 0.0070 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON CD0001 PS
LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was ..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER
Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Time 86400 sec
0.0050 - 0.0070 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP DX06411H PC
LNP* THERMOCOMP* DX06411H is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Healthcare.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 4.00 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.157 in
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin
Thin-wall injection moldings grade of high fluidity. It has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Comparatively large-size components of mechanic..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 4.00 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.157 in
Teijin Panlite® L-1225Z100 Transparent and Weather Resistant grade Polycarbonate Resin
Conforms to SAE regulations. It is an injection molding grade that has slightly high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear colorApplications:Co..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 4.00 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.157 in
Teijin Panlite® LN-2250Y Flame Resistant, Translucent Polycarbonate Resin
Flame retardant and mold release grade with normal fluidity, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications.Applications:Electric,..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 4.00 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.157 in
Teijin Panlite® LV-2225Y Standard (mold release/ice color grade) Polycarbonate Resin
Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required to be slightly high fluidity.Appl..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Ultem 1010KM PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Time 86400 sec
0.0050 - 0.0070 in/in
<br>@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific)
Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 4.00 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.157 in
Teijin Panlite® K-1300Y Standard (mold release/ice color grade) Polycarbonate Resin
Extrusion molding, blow molding and thick-wall injection molding grade. It has a improved mold release property and is bluish-tinted to exhibit clear color.Applications:Extruded products such as she..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.00 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® FR3005 BBS310 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.00 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.118 in
150x105x3mm; b.o. ISO 2577
Covestro Bayblend® FR3010 HF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
E-Polymers TEKAPPO® JF2 Un-Reinforced Heat Resistant Chemical Resistance M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
<br>@Thickness 3.20 mm
0.0050 - 0.0070 in/in
<br>@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East)
FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe..