| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
|
Lanxess Durethan® DP AKV 30 FN00 000000 Nylon 66, 30% Glass Fiber
PA 66, injection molding 30% glass fibers, UL 94 V-0 at 0.4 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, free from halogen and red phosphorous
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
|
Lanxess Pocan® TP 740-101 000000 PBT + ASA, 15% Glass Fiber
PBT+ASA, 15% glass fibers, injection molding, low tendency to warp, improved surface finish
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | |
|
LATI Latigray 82-04 CX/90 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | |
|
LATI Latishield 66-10A H2 CETG/400 PA66, Steel/Glass Fiber Reinforced, Mineral Filled, Heat Stabilized
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0070
-
0.0090
cm/cm <br>@Time 86400 sec
|
0.0070
-
0.0090
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL003EXJ PC
LNP* Lubricomp* DL003EXJ is a compound based on Polycarbonate containing 15% PTFE. Characteristics of this grade are Easy Molding, Low Extractable, Internally Lubricated, Healthcare.
|
|||
| Linear Mold Shrinkage, Transverse |
0.0070
cm/cm <br>@Time 86400 sec
|
0.0070
in/in <br>@Time 24.0 hour
|
ASTM D 955 |
|
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR
LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | ISO DIS 294-4 |
|
Wellman Wellamid® GF1662-GY1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | ISO DIS 294-4 |
|
Wellman Wellamid® GF1750-N2 50% Glass Fiber Reinforced Nylon 6
Description: Glass Fiber Reinforced Nylon 6Information provided by Wellman.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | ISO DIS 294-4 |
|
Wellman Wellamid® GF33-66/6 XE-NBK1 33% Glass Fiber Reinforced Nylon 66/6
Description: Glass Fiber Reinforced Nylon 66/6Information provided by Wellman.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | DIS 294-4 |
|
Wellman Wellpet® MRGF101-GY1 PET, 29% Mineral/Glass Fiber Reinforced
Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
|
Covestro Makrolon® 1899* Polycarbonate, Impact Grade
Formerly Makrolon DP1-1899MVR (300 °C/1.2 kg) 15.5 cm³/10 minspecial flame retardant systemUL 94V-0/0.75 mmImpact modifiedMedium viscosityEasy releaseVicat softening temperature 50 N; 50 °C/h = 1..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0070
cm/cm <br>@Thickness 2.00 mm
|
0.0070
in/in <br>@Thickness 0.0787 in
|
60x60x2 mm; 500 bar; ISO 294-4 |
|
Covestro Makrolon® 2407 MAS145 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
|
Covestro Makrolon® 2556 Polycarbonate
MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content
|
|||
| Linear Mold Shrinkage, Transverse |
0.0070
cm/cm <br>@Thickness 2.00 mm
|
0.0070
in/in <br>@Thickness 0.0787 in
|
60x60x2 mm; 500 bar; ISO 294-4 |
|
Covestro Makrolon® 2600 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4,2577 |
|
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® EBGM-20 HX PA666-GF15
Product description: Grilon EBGM-20 HX black 9992 is a high viscosity, high heat stabilized PA66 + PA6 extrusion blow molding grade with 15% glass fibers. The special features of Grilon EBGM-20 HX b..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® LV-15H nat PA12-GF15
Product description: Grilamid LV-15H is a 15% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptiongood dimension..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR
Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline P..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Rynite® FR531 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**)
36% Reinforced Flame Retardant Polyethylene Terephthalate Information provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | Eurotec |
|
Eurotec® Tecodur® PB70 GR30 NL MB04 PBT/ASA, 30% glass fiber reinforced, heat & UV stabilized, natural
Information provided by Eurotec®
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | |
|
E-Polymers SEPAZ® V240A 40% Glass Fiber Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | b.o. ISO 2577 |
|
Covestro Makroblend® UT5205 PC/PBT Blend
Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | |
|
E-Polymers TEKAMID® H14HR High Toughness Heat Resistance PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.0080 cm/cm | 0.0070 - 0.0080 in/in | ASTM D955 |
|
LNP Lubricomp® QFL-4036 BK8-115 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(disconti
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0070
-
0.0090
cm/cm <br>@Time 86400 sec
|
0.0070
-
0.0090
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC
LNP LUBRICOMP* DL002 is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | |
|
LATI Latigray 82-05 CX/90 PA 12
Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0070 - 0.0080 cm/cm | 0.0070 - 0.0080 in/in | ASTM D955 |
|
LNP Lubricomp® QFL-4017 ER HS Polyamide 6/10 Copolymer, Glass Fiber Reinforcement, PTFE Lubricant
(discontinu
Features: Heat Stabilized, Good Mold Release, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; ..
|
|||
| Linear Mold Shrinkage, Transverse |
0.0070
-
0.0090
cm/cm <br>@Thickness 3.20 mm
|
0.0070
-
0.0090
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific)
Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg..
|
|||