| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
|
Plastcom SLOVAMID 6 GF 50 LTS PA6, 50% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
|
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade
Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
|
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
|
Solvay Specialty Polymers Lavanta® 5115 WH224 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | ASTM D955 |
|
Shinkong Synthetic Fibers Shinite® N602G6S Nylon 66, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
|
|||
| Linear Mold Shrinkage, Transverse |
0.012
cm/cm <br>@Time 86400 sec
|
0.012
in/in <br>@Time 24.0 hour
|
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Linear Mold Shrinkage, Transverse |
0.012
-
0.016
cm/cm <br>@Thickness 3.20 mm
|
0.012
-
0.016
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
|
|||
| Linear Mold Shrinkage, Transverse |
0.012
-
0.016
cm/cm <br>@Thickness 3.20 mm
|
0.012
-
0.016
in/in <br>@Thickness 0.126 in
|
SABIC Method |
|
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | DIS 294-4 |
|
Wellman Wellamid® 42L-XE-N Nylon 6, Engineering Grade
All information provided by Wellman Engineered Resins.
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 |
|
DSM Akulon® S223-G4U (Cond.) 23% Glass Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® L 20A Z PA12
Product Description: Grilamid L 20A Z is a medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20A Z is impact modified, hydrolysis-and heat stabilized. Grilamid L 20A Z is used for p..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® L 25 W 40 X PA12-I
Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Crastin® SK645FR BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR BK851 is a flame retardant 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | annealed; ISO 294-4 |
|
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Eurotec |
|
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural
Information provided by Eurotec®
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® L 25 W 10 H X PA12
Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Hytrel® G4078LS NC010 Polyester Elastomer TPC-ET
(Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Light ProtectionInformation provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 2577 |
|
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**)
47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**)
13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
|
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced
15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
|
Azoty Tarnow™ Tarnamid® T-27 GF25 Polyamide 6 - Glass Fiber Reinforced
25% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Sheet |
|
BASF Ultradur B 4406 G4 PBT
Description: Is a PBT, flame-retardant injection-molding grades, with 20% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh..
|
|||
| Linear Mold Shrinkage, Transverse |
0.012
cm/cm <br>@Thickness 4.00 mm,<br> Time 86400 sec
|
0.012
in/in <br>@Thickness 0.157 in,<br> Time 24.0 hour
|
|
|
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Eurotec |
|
Eurotec® Tecomid® NB40 NL E PA6, unfilled, natural
Information provided by Eurotec®
|
|||
| Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Sheet |
|
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET
Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, ..
|
|||
| Linear Mold Shrinkage, Transverse |
0.012
cm/cm <br>@Thickness 3.20 mm
|
0.012
in/in <br>@Thickness 0.126 in
|
|
|
Unitika EX-1020K PA6, Dry
Conducting nylonInformation provided by Unitika Ltd.
|
|||