| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | STN EN ISO 294-4 |
|
Plastcom PLASTAMID® 6 GF 25 002 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 25% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, ..
|
|||
| Linear Mold Shrinkage, Transverse |
0.013
cm/cm <br>@Thickness 3.17 mm
|
0.013
in/in <br>@Thickness 0.125 in
|
ASTM D955 |
|
Network Polymers Softflex® 5300
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | 390°C nozzle, 200°C tool; ISO 294-4 |
|
Victrex® PEEK 600G Polyetheretherketone
(discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
|
|||
| Linear Mold Shrinkage, Transverse |
0.013
cm/cm <br>@Thickness 2.00 mm
|
0.013
in/in <br>@Thickness 0.0787 in
|
DAM; ISO 294-4 |
|
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**)
Zytel® 103FHS BKB038 is a heat stabilized, lubricated, PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Transverse |
0.013
cm/cm <br>@Thickness 2.00 mm
|
0.013
in/in <br>@Thickness 0.0787 in
|
DAM; ISO 294-4 |
|
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**)
Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | 410°C nozzle, 220°C mold |
|
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | |
|
Solvay TECHNYL® C 216 PA6, DRY
Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA
Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
|
Teknor Apex Monprene® MP 1187 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Linear Mold Shrinkage, Transverse |
0.013
cm/cm <br>@Thickness 2.00 mm
|
0.013
in/in <br>@Thickness 0.0787 in
|
TPE Method |
|
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding
Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | at 93°C for 30 min. |
|
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | at 93°C for 30 min. |
|
Teknor Apex TEKRON® 4300-D88F Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Linear Mold Shrinkage, Transverse |
0.013
cm/cm <br>@Thickness 3.20 mm
|
0.013
in/in <br>@Thickness 0.126 in
|
|
|
Unitika A1030BRL PA6, Dry
Information provided by Unitika Ltd.
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | |
|
Toyobo ECOVYLOPET® EMC2301 PET Bottle Recycling Grade, 15% Filler Reinforced
Features: PET Bottle Recycling Grade, 15% Filler Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | |
|
Toyobo Vylopet® EMC405A PET/PBT Blend
Key Feature: HB UL-94 ClassApplications: glossy surface componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, hi..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
|
DSM Novamid® 1013G15 1 NA PA6-GF15
15% Glass Reinforced, Injection Molding
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
|
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | DAM; ISO 194-4 |
|
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 194-4 |
|
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | Eurotec |
|
Eurotec® Tecomid® NA40 GR13 NL100 MB PA6.6, 13% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
|
Barlog Plastics KEBAPEAK XS1700 PEEK, unreinforced
PEEKInformation provided by BARLOG plastics GmbH.
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
|
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Conditioned, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ASTM D955 |
|
BLUESTAR 101G20 PBT, 20% Glass Filled
Typical Applications: Appliances, molded partsInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | STN 64 0808 |
|
Plastcom SLOVALEN PH 51 T 20 Polypropylene Homopolymer, 20% Mineral Filled
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**)
Unreinforced Polyamide 66Zytel 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | 390°C nozzle, 200°C tool; ISO 294-4 |
|
Victrex® PEEK 650G Polyetheretherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**)
Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D..
|
|||
| Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in | ISO 294-4 |
|
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)
(Unverified Data**)
Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This ..
|
|||