Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.018 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.017 - 0.018 cm/cm
0.017 - 0.018 in/in
ASTM D955
PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Thickness 3.18 mm
0.016 - 0.018 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125" bars; ASTM D955
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Thickness 3.20 mm
0.016 - 0.018 in/in

@Thickness 0.126 in
5" x 0.5" x 0.125" bar; ASTM D955
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res..
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm
0.016 - 0.018 in/in
LATI Latene® 11 MDT05-01 PP Homopolymer
Polypropylene homopolymer (PPh) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr..
Linear Mold Shrinkage, Transverse 0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
LATI Later 4-V0HF1 PBT, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Americ..
Linear Mold Shrinkage, Transverse 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
LATI Latiblend 5262 PP Homopolymer/PA6
Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Linear Mold Shrinkage, Transverse 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
LATI Latigray 47/1-01 CX/45 PP Copolymer
Radiopaque compound based on Polypropylene copolymer (PPc). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..
Linear Mold Shrinkage, Transverse 0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
LATI Latistat 45/7-02 HDPE
Dissipative product based on High density polyethylene (HD-PE). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria..
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Thickness 3.18 mm
0.016 - 0.018 in/in

@Thickness 0.125 in
ASTM D955
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea..
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Thickness 3.18 mm
0.016 - 0.018 in/in

@Thickness 0.125 in
ASTM D955
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear..
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East)
VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils.
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East)
Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g..
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East)
VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures.
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East)
VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin.
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East)
Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East)
VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance.
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Thickness 3.20 mm
0.016 - 0.018 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 6620 PBT+PC
PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Thickness 3.20 mm
0.016 - 0.018 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Xenoy® 6620U PBT+PC
PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance.
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Linear Mold Shrinkage, Transverse 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
DIS 294-4
Wellman Wellamid® MRT1487 BK Nylon 66, 32% Mineral Reinforced
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Transverse 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
DIS 294-4
Wellman Wellamid® MRT1487 N Nylon 66, 32% Mineral Reinforced, Impact Modified
All information provided by Wellman Engineered Resins.
Linear Mold Shrinkage, Transverse 0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
LATI Latimass 53/11-02 D030 PP Homopolymer, Impact Modified
Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation..
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East)
VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes.
Linear Mold Shrinkage, Transverse 0.0090 - 0.018 cm/cm
0.0090 - 0.018 in/in
on tensile bar; SABIC Method
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East)
VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI..
Copyright © lookpolymers.com All Rights Reserved