Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.020 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ASTM E831
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, Dry As Molded  (discontinued **)
AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist..
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
Aardvark Polymers AARTEL® 100 D/S Rotational Molding Resin
Aartel 100SD is a new conductive grade developed to dissipate electricity in fuel handling systems. Aartel 100SD maintains all o the excellent properties of our general purpose acetal, has a volume ..
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ASTM D955
LG Chemical Lupox® GP-1001F General Purpose PBT, Unreinforced, Flame Retardant
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Linear Mold Shrinkage, Transverse 0.020 - 0.0225 cm/cm
0.020 - 0.0225 in/in
LATI Latan 23UV POM
Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by ..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12
LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP
LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 - 0.021 cm/cm

@Time 86400 sec
0.020 - 0.021 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific)
LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.020 - 0.021 cm/cm

@Time 86400 sec
0.020 - 0.021 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT
LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT
LNP* LUBRICOMP* WL003 is a compound based on PBT resin containing 15% PTFE. Added feature of th is grade is: Wear Resistant.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP KF006 Acetal Copoly
LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. Added features of this material include: Chemically Coupled.
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
SABIC Method
SABIC Innovative Plastics LNP Thermocomp MX01767C PP
LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB..
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT
LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon IS000LX PA6.12
LNP* Stat-Kon* IS000LX is a compound based on Nylon 6/12 containing Stainless Steel Fibers.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE)
LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber.
Linear Mold Shrinkage, Transverse 0.020 - 0.024 cm/cm
0.020 - 0.024 in/in
ISO DIS 294-4
Wellman Wellamid® 22L-NBK1 Engineering Grade Nylon 66
Description: Engineering Grade Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.020 - 0.025 cm/cm
0.020 - 0.025 in/in
ISO DIS 294-4
Wellman Wellamid® XT1867-BK1 High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
DSM Novamid® ST120 NAT PA6-I
Impact Modified, Injection Molding
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
DSM Novamid® ST220 NAT PA6-I
Impact Modified, Injection Molding, Medium Viscosity
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
Eurotec
Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
Barlog Plastics KEBAFORM C 130.2 POM Copolymer unreinforced
POMInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
Barlog Plastics KEBAFORM C 90 W POM Copolymer unreinforced, drinking water approved
POMInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
Barlog Plastics KEBAFORM C 90.0 POM Copolymer unreinforced
POMInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Transverse 0.020 cm/cm
0.020 in/in
ISO 294-4
Barlog Plastics KEBAFORM C 901 VT POM Copolymer unreinforced, antistatic
POMInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Diameter 2.00 mm
0.020 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, Conditioned
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Thickness 2.00 mm
0.020 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Thickness 2.00 mm
0.020 in/in

@Thickness 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 67B Nylon 66, General Purpose, very high viscosity, DAM
Vydyne® 67B is a very-high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67B resin offers high strength, rigidity and..
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Diameter 2.00 mm
0.020 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, Conditioned
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
Linear Mold Shrinkage, Transverse 0.020 cm/cm

@Diameter 2.00 mm
0.020 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
Copyright © lookpolymers.com All Rights Reserved