| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Transverse | 0.010 - 0.021 cm/cm | 0.010 - 0.021 in/in | Flame Bar; ASTM D955 |
|
DSM Biomedical PurSil® 10 Thermoplastic Silicone Polyether Urethane
(discontinued **)
PurSil® thermoplastic siliconepolyether-urethane (TSPU) is a novel copolymer that is strong, yet flexible with proven biocompatibility and biostability. Leveraging the benefits of both silicone ela..
|
|||
| Linear Mold Shrinkage, Transverse | 0.0185 - 0.021 cm/cm | 0.0185 - 0.021 in/in | |
|
LATI Latan 13 S/20 POM, 20% Glass Bead Reinforced
Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro..
|
|||
| Linear Mold Shrinkage, Transverse |
0.020
-
0.021
cm/cm @Time 86400 sec |
0.020
-
0.021
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66
LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant.
|
|||
| Linear Mold Shrinkage, Transverse |
0.020
-
0.021
cm/cm @Time 86400 sec |
0.020
-
0.021
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific)
LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.020
-
0.021
cm/cm @Time 86400 sec |
0.020
-
0.021
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated.
|
|||
| Linear Mold Shrinkage, Transverse |
0.020
-
0.021
cm/cm @Time 86400 sec |
0.020
-
0.021
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant.
|
|||
| Linear Mold Shrinkage, Transverse |
0.020
-
0.021
cm/cm @Time 86400 sec |
0.020
-
0.021
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific)
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized.
|
|||
| Linear Mold Shrinkage, Transverse |
0.020
-
0.021
cm/cm @Time 86400 sec |
0.020
-
0.021
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Linear Mold Shrinkage, Transverse | 0.019 - 0.021 cm/cm | 0.019 - 0.021 in/in | ASTM D955 |
|
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
Amodel® AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40..
|
|||
| Linear Mold Shrinkage, Transverse | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO DIS 294-4 |
|
Wellman Wellamid® 22L-BL Engineering Grade Nylon 66
Description: Engineering Grade Nylon 66Information provided by Wellman.
|
|||
| Linear Mold Shrinkage, Transverse | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO DIS 294-4 |
|
Wellman Wellamid® NB1803E-BK Nylon/Polypropylene Alloy
Description: Nylon/Polypropylene AlloyInformation provided by Wellman.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.021
cm/cm @Time 86400 sec |
0.019
-
0.021
in/in @Time 24.0 hour |
ISO 294 |
|
Eurostar Staramide P1000EI3 PA6, Impact Modified, Injection Molded
Staramide P1000EI3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020)Information provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Transverse | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ISO DIS 294-4 |
|
Wellman Wellamid® XT1863-BK1 Impact Modified Nylon 66
Description: Impact Modified Nylon 66Information provided by Wellman.
|
|||
| Linear Mold Shrinkage, Transverse | 0.019 - 0.021 cm/cm | 0.019 - 0.021 in/in | ASTM D955 |
|
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**)
Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), ..
|
|||
| Linear Mold Shrinkage, Transverse | 0.019 - 0.021 cm/cm | 0.019 - 0.021 in/in | ISO 294-4 |
|
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion
(discontinued **)
AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil..
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.021
cm/cm @Time 86400 sec |
0.019
-
0.021
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP Thermotuf P1000EI3 PA 6 (Asia Pacific)
High Impact Nylon 6 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Transverse |
0.019
-
0.021
cm/cm @Time 86400 sec |
0.019
-
0.021
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP Thermotuf P1000EI3 PA 6 (Europe-Africa-Middle East)
High Impact Nylon 6 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Linear Mold Shrinkage, Transverse | 0.0175 - 0.021 cm/cm | 0.0175 - 0.021 in/in | |
|
LATI Latilub 73/13 Y/20 POM, 20% Aramid Fiber Reinforced
Self-lubricating product based on Polyoxymethylene (POM). Aramid fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
|
|||