Polymer Property : Linear Mold Shrinkage = 0.0080 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0080 cm/cm

@Thickness 6.40 mm
0.0080 in/in

@Thickness 0.252 in
Transverse; DAM
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.0080 - 0.014 cm/cm

@Thickness 1.60 mm
0.0080 - 0.014 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 4130-104D 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.0080 - 0.016 cm/cm

@Thickness 1.60 mm
0.0080 - 0.016 in/in

@Thickness 0.0630 in
horizontal; ASTM D955
Gromax PBT 2100-104B
Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen..
Linear Mold Shrinkage 0.0080 - 0.014 cm/cm

@Thickness 1.60 mm
0.0080 - 0.014 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 3030-104 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
72 hr; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.011 cm/cm

@Thickness 3.00 mm
0.0080 - 0.011 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0080 - 0.013 cm/cm

@Thickness 3.00 mm
0.0080 - 0.013 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm

@Thickness 3.20 mm
0.0080 - 0.012 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 555-31 Recycled Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.0080 cm/cm

@Thickness 1.60 mm
0.0080 in/in

@Thickness 0.0630 in
Flow; DAM
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance..
Linear Mold Shrinkage 0.0080 cm/cm

@Thickness 1.60 mm
0.0080 in/in

@Thickness 0.0630 in
Transverse; DAM
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance..
Linear Mold Shrinkage 0.0080 cm/cm

@Thickness 1.60 mm
0.0080 in/in

@Thickness 0.0630 in
Transverse; DAM
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66
Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.0080 - 0.014 cm/cm

@Thickness 1.60 mm
0.0080 - 0.014 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.0080 - 0.014 cm/cm

@Thickness 1.60 mm
0.0080 - 0.014 in/in

@Thickness 0.0630 in
vertical; ASTM D955
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..