Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.011 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.20 mm
0.011 in/in

@Thickness 0.126 in
Transverse; DAM
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.20 mm
0.011 in/in

@Thickness 0.126 in
Flow; DAM
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.20 mm
0.011 in/in

@Thickness 0.126 in
Transverse; DAM
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Zytel® 151 NC010 is a PA 612 resin.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/CC/40 Polypropylene Homopolymer, 40% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.011 - 0.012 cm/cm

@Thickness 6.35 mm
0.011 - 0.012 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.011 - 0.014 cm/cm

@Thickness 3.17 mm
0.011 - 0.014 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 6.35 mm
0.011 in/in

@Thickness 0.250 in
ASTM D955
Fiberfil® PP-60/CC/30 Polypropylene Homopolymer, 30% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.17 mm
0.011 in/in

@Thickness 0.125 in
ASTM D955
Fiberfil® PP-60/CC/30 Polypropylene Homopolymer, 30% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 - 0.016 cm/cm

@Thickness 3.20 mm
0.011 - 0.016 in/in

@Thickness 0.126 in
48 hr, at 121°C; ASTM D955
A. Schulman POLYPUR™ FPU 1109 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Linear Mold Shrinkage 0.011 cm/cm

@Temperature 240 °C
0.011 in/in

@Temperature 464 °F
ASTM D3392
DuPont™ Nomex® Type 993, 40 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Linear Mold Shrinkage 0.011 cm/cm

@Temperature 240 °C
0.011 in/in

@Temperature 464 °F
ASTM D3392
DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 6.40 mm
0.011 in/in

@Thickness 0.252 in
Transverse; DAM
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612
Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.20 mm
0.011 in/in

@Thickness 0.126 in
Flow; DAM
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance..
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.20 mm
0.011 in/in

@Thickness 0.126 in
Transverse; DAM
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance..
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 1.60 mm
0.011 in/in

@Thickness 0.0630 in
Transverse; DAM
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.011 cm/cm

@Thickness 3.20 mm
0.011 in/in

@Thickness 0.126 in
Flow; DAM
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612  (Unverified Data**)
Zytel® FE3734 NC010 is an unreinforced, lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.011 - 0.015 cm/cm

@Thickness 3.20 mm
0.011 - 0.015 in/in

@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
A. Schulman FORMION™ FI 389 Ionomer
Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved