Polymer Property : Melt Index of Compound = 0.50 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Melt Index of Compound 0.50 - 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 - 0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film
The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng..
Melt Index of Compound 0.50 - 0.70 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 - 0.70 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film
The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE  (discontinued **)
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE  (discontinued **)
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPEHigh a..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Polykemi AB POLYfill PPC 05ENH Polypropylene Copolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
Melt Index of Compound 0.50 - 0.80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 - 0.80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Petroquimica Triunfo Tritheva® TN 2007 EVA Copolymer
The Tritheva TN 2007 resin is an Ethylene-Vinyl Acetate copolymer (EVA), developed to meet the multi-layer packaging needs where are required high strength, with high toughness, and excellent optica..
Melt Index of Compound 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Lushan PJ-1 Polypropylene Compounds for Steel Pipe Top Coats
Polypropylene compound for steel pipe top coats Lushan PJ-1 is used for 3LPP coating system in colored white. It is supplied in pellets for melt extrusion or in a powder for application by spray or ..
Melt Index of Compound 0.50 g/10 min
0.50 g/10 min
ASTM D1238
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Melt Index of Compound 0.50 g/10 min
0.50 g/10 min
ASTM D1238
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Melt Index of Compound 0.50 g/10 min
0.50 g/10 min
ASTM D1238
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Melt Index of Compound 0.50 g/10 min

@Temperature 230 °C
0.50 g/10 min

@Temperature 446 °F
ASTM D1238
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability
Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo.
Melt Index of Compound 0.50 g/10 min
0.50 g/10 min
ASTM D1238
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: High strengthGood drawdownGood processabilityUse alone or in blends with LDPE or HDPE Appl..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow Engage® 8150 Polyolefin Elastomer
Description: Engage® 8150 and Engage® 8157 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and provide good impact properties in blends with polypropy..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow Engage® 8157 Polyolefin Elastomer
Description: Engage® 8157 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow Engage® 8180 Polyolefin Elastomer
Description: Engage® 8180 polyolefin elastomer is a lower density, high performance ethylene-octene copolymer that has excellent flow characteristics and provides good impact properties in blends w..
Melt Index of Compound <= 0.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 0.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Dynasol Solprene® 412 Thermoplastic Elastomer
Solprene 412 is a radial oil extended styrene butadiene block copolymer having 30% of styrene content, most of it forming a polystyrene block which gives the polymer a thermoplastic behavior. It is ..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Arkema Group OREVAC® 18630 Maleic Anhydride Modified Ethylene - Acrylate Copolymer
OREVAC® 18630 is anhydride modified Ethylene – Acrylate copolymer. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) ..
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Braskem INSPIRE™ 114 Performance Polypropylene Polymer
OverviewHigh melt strengthHigh toughnessExcellent processabilityHigh impact and puncture resistanceHigh film stiffness/machinabilityHigh heat resistanceComplies with U.S. FDA FCN 843, Europe EU-Dire..
Melt Index of Compound <= 0.50 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 0.50 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
Dynasol Solprene® 416 Thermoplastic Rubber SBS Dry
Solprene 416 is a radial styrene/butadiene block copolymer having 30% of styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops proper..
Melt Index of Compound 0.50 g/10 min
0.50 g/10 min
ASTM D1238
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..
Melt Index of Compound 0.50 g/10 min
0.50 g/10 min
ASTM D1238
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains ..