| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Index of Compound |
3.0
g/10 min @Load 5.00 kg, Temperature 230 °C |
3.0
g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
|
Polykemi AB POLYabs XX0 ABS, Extrusion Grade
Information provided by Polykemi AB
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Polykemi AB POLYfill PPH GF3045 HC Polypropylene Homopolymer, Glass Fibre-Reinforced
Information provided by Polykemi AB
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Polykemi AB POLYfill PPH GF3050 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Polykemi AB POLYfill PPHC GF3030 PD2 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0
g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
|
SABIC Innovative Plastics Lexan® 133R PC (Europe-Africa-Middle East)
LEXAN 133R is the highest viscosity, UV stabilized, release containing, linear polycarbonate grade. Suitable for injection molding and extrusion processes. Available in transparent and multiple colo..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0
g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
|
SABIC Innovative Plastics Lexan® 134R PC (Europe-Africa-Middle East)
LEXAN 134R is a high viscosity grade especially suited for injection blow moulding. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade will no longer be supported..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0
g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
|
SABIC Innovative Plastics Lexan® 4504 PPC
High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with ..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
|
Polykemi AB POLYform POM C M20 AS4 Polyoxymethylene, Antistatic
Information provided by Polykemi AB
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 5.00 kg, Temperature 372 °C |
3.0
g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
|
3M Dyneon™ PFA 6503 A EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **)
Dyneon PFA 6503 A EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 5.00 kg, Temperature 372 °C |
3.0
g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
|
3M Dyneon™ PFA 6503 C EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **)
Dyneon PFA 6503 C EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
ICO Polymers ICORENEâ„¢ 155-1339 LMDPE Rotational Molding Resin
Description: ICORENE 155-1339 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Temperature 230 °C |
3.0
g/10 min @Temperature 446 °F |
ASTM D1238 |
|
Mitsui ADMER® QB510A PP Type Polyolefin
ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Temperature 230 °C |
3.0
g/10 min @Temperature 446 °F |
ASTM D1238 |
|
Mitsui ADMER® QF500A PP Type Polyolefin
ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Temperature 190 °C |
3.0
g/10 min @Temperature 374 °F |
ASTM D1238 |
|
Mitsui ADMER® NF498A PE Type Polyolefin
ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 5.00 kg, Temperature 280 °C |
3.0
g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
|
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific)
PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications.
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 265 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 265 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
|
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 5.00 kg, Temperature 260 °C |
3.0
g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
|
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East)
PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP..
|
|||
| Melt Index of Compound | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
|
DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
|
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE
Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Dow Engage® 8450 Polyolefin Elastomer
Description: Engage® 8450 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Dow Engage® 8452 Polyolefin Elastomer
Description: Engage® 8452 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent toughness, softness, and optical properties. It has excellent compatibility with other polyolefin..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Arkema Group LOTADER® TX 8030 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER TX 8030 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER TX 8030 is an adhesive designed for extrusion coating ..
|
|||
| Melt Index of Compound |
3.0
-
4.5
g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0
-
4.5
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Arkema Group EVATANE® 28-03 Copolymer Ethylene - Vinyl Acetate
EVATANE® 28-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-03 is stabilized with antioxidants. The High Vinyl Acetate co..
|
|||
| Melt Index of Compound |
3.0
-
4.0
g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0
-
4.0
g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
|
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification
The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Polykemi AB POLYfill PP TOUCH 34725 Polypropylene, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0
g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
|
Polykemi AB POLYfill PPH TS3020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Melt Index of Compound | 3.0 g/10 min | 3.0 g/10 min | |
|
Lushan OR-1 Halogen-Free Flame-Retardant Compatibilizer
Halogen-free flame retardant compatibilizer Lushan series for cables and wires are developed by several doctors and maters from Lushan’s R&D Center, and combined ten years’ modified polyolefin gra..
|
|||
| Melt Index of Compound |
3.0
g/10 min @Load 5.00 kg, Temperature 372 °C |
3.0
g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
|
3M Dyneon™ PFA 6503 B EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **)
Dyneon PFA 6503 B EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick ..
|
|||