Polymer Property : Viscosity = 1.00e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 30.0 - 1.00e+6 cP
30.0 - 1.00e+6 cP
Average value: 45700 cP Grade Count:45
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Viscosity 300000 - 1.00e+6 cP
300000 - 1.00e+6 cP
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Viscosity 300000 - 1.00e+6 cP
300000 - 1.00e+6 cP
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Viscosity 300000 - 1.00e+6 cP
300000 - 1.00e+6 cP
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..