Polymer Property : Viscosity = 1.05e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 1.05e+6 cP

@Temperature 160 °C
1.05e+6 cP

@Temperature 320 °F
Melt; ISO 1133
Lubrizol Advanced Materials Pearlbond® 12C75 Thermoplastic Polyurethane
Pearlbond® 12C75 is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low softe..
Viscosity 1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Akulon® F130 PA6
Film Extrusion, Medium Viscosity
Viscosity 1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Akulon® F130-C PA6
Film Extrusion, Medium Viscosity, Lubricated
Viscosity 1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
Viscosity 1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Viscosity 1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
Viscosity 1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 240 °C
1.05e+6 cP

@Shear Rate 0.100 1/s,
Temperature 464 °F
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock