Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 100 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 100 - 200 cP

@Temperature 25.0 °C
100 - 200 cP

@Temperature 77.0 °F
Uncured
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Viscosity 100 cP
100 cP
Resinlab® CYNERGY CA6005 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Viscosity 100 cP
100 cP
Resinlab® CYNERGY CA6103 Adhesive
Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates..
Viscosity 100 cP
100 cP
Resinlab® CYNERGY CA6702 Adhesive
Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal ..
Viscosity 100 - 15000 cP

@Temperature 45.0 - 82.2 °C
100 - 15000 cP

@Temperature 113 - 180 °F
Average value: 2520 cP Grade Count:8
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Viscosity 100 cP
100 cP
Part A (Isocyanate), RVT, #2, 20 rpm; TM R050-12
Resinlab® UR3001HP Black Urethane Encapsulant
Resinlab™ UR3001HP Black is a black, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Black provides excellent e..
Viscosity 100 - 180 cP
100 - 180 cP
LG Chemical CP-HR Polycarboxylic Copolymer
Description: Advantages: CP-HR is the main raw material for concrete admixture, which improves water reducing ability of Ultra high strength concrete. CP-HR exhibits superior properties of High stor..
Viscosity 100 - 200 cP
100 - 200 cP
As Supplied
Heraeus Cleviosâ„¢ P T2 Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P T2 is an antistatic material based on PEDOT:..
Viscosity <= 100 cP
<= 100 cP
Solvay Specialty Polymers Solvera® PT 5071 PFPE Surface Treatment
Solvera® PFPE is a sustainable surface treatment developed to increase the grease resistance of paper packaging, pizza boxes, popcorn bags, pet food bags and food wraps. Both solvent and aqueous..
Viscosity 100 - 800 cP
100 - 800 cP
ASTM D803
SK Chemicals SKYTHANE® UB220 Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Viscosity <= 100 cP
<= 100 cP
Solvay AG-RHOâ„¢ GPA Surfactant
Description: Ag-RHO GPA is a surfactant for pesticide formulations. It is a bioactivator that can be used to replace alky polyglucosides (APG's) in aqueous formulations, tank mix adjuvants, and liqu..
Viscosity <= 100 cP
<= 100 cP
Cannon Fenske at 40°C; RPG62
Solvay GEROPON® T/36 DF Surfactant
Identification: SODIUM POLYCARBOXYLATE, AQUEOUS SOLUTION. Solubility: Soluble in water. Insoluble in polar and aromatics solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaA..
Viscosity 100 - 200 cP
100 - 200 cP
NOV QC 020
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Viscosity 100 cP

@Temperature 200 °C
100 cP

@Temperature 392 °F
Melt
Unitika elitel UE3700 Polyester, Pellet
Hot melt adhesives, Adhesives for fibers, Adhesives for interlining clothsUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from p..
Viscosity <= 100 cP
<= 100 cP
Dynamic
Dow Corning 9011 Silicone Elastomer Blend
A dispersion of high molecular weight silicone elastomer substituted with polyether in cyclopentasiloxane for use in skincare, suncare, color cosmetics, and antiperspirant / deodorant applications.I..
Viscosity 100 cP
100 cP
Dynamic
Dow Corning SYL-OFF® PMCPSL 8 Crosslinker
Syl-Off SL 8 Crosslinker is very fast cure (contains mist reduction additive)Information provided by Dow Corning
Viscosity 100 cP
100 cP
dynamic
Dow Corning SYL-OFF® SL 8 CROSSLINKER
Solvent-free, fast curing, actively reduces mist at high speeds, good balance of cure and anchorage performanceInformation provided by Dow Corning
Viscosity 100 cP
100 cP
ACC EP MAP-18 EPI Engineered Polymers Aliphatic Polymer
EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-18 contains 18% NCO. Pa..
Viscosity 100 cP
100 cP
Hardener
ACC EP QSZ EPI Engineered Polymers Quick Set Epoxy with Zinc
EP QSZ Quick Set Epoxy with Zinc, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC’s (Volatile Organic Compound), self-leveling modified epoxy. This versatile new gene..
Viscosity 100 cP
100 cP
Uncatalyzed, QM CAT PURPLE
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material
QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us..
Viscosity 100 cP
100 cP
Uncatalyzed, QM CAT PURPLE
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material
QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili..
Viscosity 100 cP
100 cP
Uncatalyzed, QM CAT SKIN 30
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material
QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l..
Viscosity 100 cP
100 cP
Uncatalyzed, QM CAT RED 3
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material
QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f..
Viscosity 100 - 250 cP
100 - 250 cP
Aremco Pyro-Paint™ 634-GR High Temperature Refractory Coating, GR >95%
This carbon and graphite based coating is formulated for parting of aluminum permanent molds, non-sticking in glass forming applications, and lubrication and stop-off in metalworking and wire drawin..
Viscosity 100 - 1500 cP
100 - 1500 cP
Beijing Ranger Chem SM-601REK70 Solvent Based Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 100 - 800 cP
100 - 800 cP
Beijing Ranger Chem SM-828A90 Solvent Based Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 100 cP
100 cP
Hardener
ACC EP QS EPI Engineered Polymers Quick Set Epoxy
EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure..
Viscosity <= 100 cP
<= 100 cP
RP-0596
Solvay RHODAPEX® ES STD Surfactant
Chemical Name: SODIUM LAURETH SULFATECAS: 68585-34-2Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX© ES STD is a primary foaming agent in shampoos, bath p..
Viscosity 100 - 300 cP
100 - 300 cP
#2 sp @ 30 rpm; RP-0596
Solvay RHODOLINE® 270 Surfactant
Description: Polyacid dispersant. Highly versatile, economical and low foam, flat to gloss, ideal for interior application.Identification: ACRYLIC POLYMERCAS: 9003-04-7Available in: North America IR..
Copyright © lookpolymers.com All Rights Reserved