| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 100 cP | 100 cP | |
|
Ritelok PR100 Plastic & Rubber Adhesive
Cyanoacrylate. Medium strength plastic & rubber adhesive. For difficult to bond rubber & plastic. High bond strength, Medium viscosity, Fast cure
|
|||
| Viscosity |
100
-
300
cP @Temperature 32.2 °C |
100
-
300
cP @Temperature 90.0 °F |
|
|
Old Hickory UltraCast Slurry PC-2000 Kentucky Ball Clay
These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c..
|
|||
| Viscosity |
100
-
300
cP @Temperature 32.2 °C |
100
-
300
cP @Temperature 90.0 °F |
|
|
Old Hickory UltraCast Slurry UC-34A Kentucky Ball Clay
These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c..
|
|||
| Viscosity | 100 - 500 cP | 100 - 500 cP | |
|
ND Industries 530 Shaft & Bearing Retainer Retaining Compound
General DescriptionA high strength adhesive for retention of cylindrical components, where disassembly is not required.Typical Usesrotors, shafts, bushings, bearings, and pulleysMeets military spec ..
|
|||
| Viscosity |
100
-
400
cP @Temperature 45.0 °C |
100
-
400
cP @Temperature 113 °F |
|
|
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity | 100 cP | 100 cP | |
|
Hybrid Plastics FireQuench® PM 1287 Resin
FireQuench® PM1287 is an optically transparent, fire retardant hybrid nanocomposite resin that can serve as a replacement for standard epoxy-vinyl ester and related resins. It can be employed as ..
|
|||
| Viscosity | 100 - 180 cP | 100 - 180 cP | |
|
LG Chemical CP-HR Polycarboxylic Copolymer
Description: Advantages: CP-HR is the main raw material for concrete admixture, which improves water reducing ability of Ultra high strength concrete. CP-HR exhibits superior properties of High stor..
|
|||
| Viscosity | <= 100 cP | <= 100 cP | |
|
KKPC KOSYN KSL 361 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 300 series is a Styrene-Butadiene Latex.Applications: Oil-resistant Foam Rubber, For Impregnation of Tire and Belt Cord, Foam Backing of Textile Goo..
|
|||
| Viscosity |
<=
100
cP @Time 60.0 sec |
<=
100
cP @Time 0.0167 hour |
#60 spindle, 60 rpm; LSY-QB-ID006 |
|
LG Chemical Lutex 105 NBR Latex
Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Softness, WhitenessApplication: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Industrial Glove..
|
|||
| Viscosity |
<=
100
cP @Time 60.0 sec |
<=
100
cP @Time 0.0167 hour |
#60 spindle, 60 rpm; LSY-QB-ID006 |
|
LG Chemical Lutex 120 NBR Latex
Description: Tensile strength, Elongation, Oil resistance, Abrasion resistance, Excellent elasticity, WhitenessApplication: Nitrile Glove (Examination Glove, Clean Room Glove), Supported Glove (Indu..
|
|||
| Viscosity | 100 cP | 100 cP | |
|
KKPC KOSYN KSL 101 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 100 series are carboxy metamorphic styrene-butadiene latexes. They have a soft touch and high adhesive force.Applications: Carpet Backing, Adhesive ..
|
|||
| Viscosity | 100 - 200 cP | 100 - 200 cP | ASTM D803 |
|
SK Chemicals SKYTHANE® US210 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Viscosity | <= 100 cP | <= 100 cP | Cannon Fenske at 40°C; RPG62 |
|
Solvay GEROPON® T/36 DF Surfactant
Identification: SODIUM POLYCARBOXYLATE, AQUEOUS SOLUTION. Solubility: Soluble in water. Insoluble in polar and aromatics solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaA..
|
|||
| Viscosity |
100
-
750
cP @Temperature 190 °C |
100
-
750
cP @Temperature 374 °F |
542-111 |
|
Westlake Epolene® E-43P Oxidized Low Molecular Weight Polyethylene Polymer
Description: Epolene E-43P is a maleic anhydride grafted polypropylene powder recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul..
|
|||
| Viscosity |
100
-
400
cP @Temperature 45.0 °C |
100
-
400
cP @Temperature 113 °F |
|
|
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity | 100 - 130 cP | 100 - 130 cP | uncured coating |
|
Master Bond UV15SP-1 Low Viscosity, UV Curable System
Description: Master Bond UV15SP-1 is a new one component, high strength UV curable epoxy resin based polymer system for bonding, sealing, & coating with high performance properties. It is a 100% rea..
|
|||
| Viscosity |
100
-
300
cP @Temperature 75.0 °C |
100
-
300
cP @Temperature 167 °F |
|
|
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity |
100
-
200
cP @Temperature 23.0 °C |
100
-
200
cP @Temperature 73.4 °F |
100 rpm |
|
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy
Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug..
|
|||
| Viscosity | 100 cP | 100 cP | |
|
ACC EP MAP-18 EPI Engineered Polymers Aliphatic Polymer
EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-18 contains 18% NCO. Pa..
|
|||
| Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT RED 3 |
|
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material
QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an..
|
|||
| Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT PURPLE |
|
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material
QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili..
|
|||
| Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT RED 3 |
|
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material
QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f..
|
|||
| Viscosity | 100 cP | 100 cP | |
|
3M Scotch-Weld™ LO100 Low Odor Instant Adhesive
3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o..
|
|||
| Viscosity | <= 100 cP | <= 100 cP | |
|
3M Dynamar™ RC 5125 Rubber Curative
3M™ Dynamar™ Rubber Curatives RC 5105, RC 5110, RC 5115, RC 5120 and RC 5125 are liquid curatives that offer fast and easy incorporation into solvent based FKM solution coatings. RC 5125 is a sila..
|
|||
| Viscosity | 100 cP | 100 cP | Hardener |
|
ACC EP QS EPI Engineered Polymers Quick Set Epoxy
EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure..
|
|||
| Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT RED 3 |
|
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material
QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an..
|
|||
| Viscosity | 100 cP | 100 cP | |
|
Resinlab® CYNERGY CA6903 Adhesive
Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials..
|
|||
| Viscosity | <= 100 cP | <= 100 cP | RP-0596 |
|
Solvay RHODAPON® OLS Surfactant
Description: Rhodapon OLS is good dispersant, wetting agent and excellent low foam detergent. It helps to reduce spots and streaksChemical Name: SODIUM OCTYL SULFATECAS: 142-31-4; 111-87-5Available ..
|
|||