| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
1000
-
1400
cP <br>@Temperature 25.0 °C
|
1000
-
1400
cP <br>@Temperature 77.0 °F
|
|
|
Northstar Polymers PND-011 Polyether Curing Agent
Information provided by Northstar Polymers.
|
|||
| Viscosity | 1000 cP | 1000 cP | Part B, RVT, #2, 2.5 rpm; TM R050-12 |
|
Resinlab® EP1385 Black Epoxy Formulation
Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w..
|
|||
| Viscosity | 1000 - 2000 cP | 1000 - 2000 cP | |
|
Huntsman Araldite ECN 1285 Epoxy Cresol Novolac
Weight per Epoxide (EEW, g/eq) 212 to 227. Amber color.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
|
|||
| Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 25% Toluene Solution at 25°C; KM 06 |
|
Kraton® D1184 A (SBS) Branched Block Copolymer
Description: Kraton D1184 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows..
|
|||
| Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% Toluene Solution at 25°C; KM 06 |
|
Kraton® D1186 B (SBS) Branched Triblock Copolymer
Description: Kraton D1186 BT is a clear, branched triblock copolymer based on styrene and butadiene with a polystyrene content of 30%. It is supplied from South America in the physical form identifi..
|
|||
| Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% Toluene Solution at 25°C; KM 06 |
|
Kraton® D1186 E (SBS) Branched Block Copolymer
Description: Kraton D1186 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows..
|
|||
| Viscosity |
1000
-
1500
cP <br>@Temperature 20.0 °C
|
1000
-
1500
cP <br>@Temperature 68.0 °F
|
|
|
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup
Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International
|
|||
| Viscosity | 1000 - 5000 cP | 1000 - 5000 cP | #3 Spindle, 12 rpm >1 min; RP-17619 |
|
Solvay MIRACARE® SLB-365/N Surfactant
Description: Surfactant blend used in the production of structured liquid formulations. The preservative in MIRACARE SLB-365/N is a non-formaldehyde donor (Neolone).I.N.C.I. Name: WATER, SODIUM TRID..
|
|||
| Viscosity | <= 1000 cP | <= 1000 cP | #3 sp @ 60 rpm; RP-0596 |
|
Solvay RHODOLINE® 581B Surfactant
Description: Mineral oil defoamers for high PVC systems Chemical Name: DEFOAMERCAS: 64742-47-8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility(2% in DI Water): Coarse Di..
|
|||
| Viscosity |
1000
-
2500
cP <br>@Temperature 125 °C
|
1000
-
2500
cP <br>@Temperature 257 °F
|
V-005 |
|
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h..
|
|||
| Viscosity |
1000
cP <br>@Temperature 25.0 °C
|
1000
cP <br>@Temperature 77.0 °F
|
After mixing |
|
Tra-Con Tra-Bond F202 Spectrally Transparent High Temperature Epoxy Adhesive
TRA-BOND F202 is a clear, low viscosity epoxy adhesive recommended for photonic applications requiring exposure to high temperatures or chemical and environmental resistance. This 100% solids system..
|
|||
| Viscosity | 1000 cP | 1000 cP | at 20 RPM |
|
Loctite® 312 Acrylic Bonding Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
|
|||
| Viscosity |
1000
cP <br>@Temperature 23.9 °C
|
1000
cP <br>@Temperature 75.0 °F
|
|
|
TSE Industries EzNATE® SS100 Aliphatic Polyurethane Resin
TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA..
|
|||
| Viscosity |
1000
cP <br>@Temperature 30.0 °C
|
1000
cP <br>@Temperature 86.0 °F
|
Liquid |
|
DSM Somos® PerFORM Stereolithography Polymer, UV Postcure
PerFORM produces strong, stiff, high-temperature resistant composite parts on standard 355 nm stereolithography machines. This material’s lower viscosity makes processing parts faster. It exhibits ..
|
|||
| Viscosity |
1000
-
3000
cP <br>@Temperature 23.0 °C
|
1000
-
3000
cP <br>@Temperature 73.4 °F
|
100 rpm |
|
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy
Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
|
|||
| Viscosity | 1000 cP | 1000 cP | |
|
Elmer's Products Aron Alpha® 403T Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
|
|||
| Viscosity | 1000 - 2500 cP | 1000 - 2500 cP | |
|
Abatron AboCast/AboCure 8109-6
High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat..
|
|||
| Viscosity |
1000
-
2000
cP <br>@Temperature 25.0 °C
|
1000
-
2000
cP <br>@Temperature 77.0 °F
|
MA143LFE |
|
C.O.I.M. FILCO® 358 Film Former for Glass Fiber Sizes
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar..
|
|||
| Viscosity | 1000 cP | 1000 cP | "B" component |
|
ACC QGel 310 QSI Quantum Silicones High Strength Gel
QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..
|
|||
| Viscosity | 1000 cP | 1000 cP | "A" component |
|
ACC QGel 311 QSI Quantum Silicones General Purpose Silicone Gel
QGel 311 is a clear, fast cure, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..
|
|||
| Viscosity | 1000 cP | 1000 cP | "B" component |
|
ACC QGel 315 QSI Quantum Silicones General Purpose Silicone Gel
QGel 315 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..
|
|||
| Viscosity |
<=
1000
cP <br>@Temperature 75.0 °C
|
<=
1000
cP <br>@Temperature 167 °F
|
|
|
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic
Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem..
|
|||
| Viscosity | 1000 - 2000 cP | 1000 - 2000 cP | |
|
Aremco Aremco-Seal™ 613 High Temperature Glass Coating
Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1150 ºF (620 ºC)
|
|||
| Viscosity | 1000 - 2000 cP | 1000 - 2000 cP | |
|
Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95%
This highly-filled zirconium oxide-based coating produces a hard, chemically-resistant protective layer which is stable with aluminum, molybdenum, platinum, rhodium, and titanium. It is ideal for se..
|
|||
| Viscosity | 1000 cP | 1000 cP | |
|
BASF Lupranate® 5060 Isocyanate
Description: Lupranate® 5060 Isocyanate is a low functional prepolymer based on monomeric MDI. Lupranate® 5060 isocyanate is suitable for use in a broad range of flexible, semi-flexible, and cast ..
|
|||
| Viscosity | 1000 - 1500 cP | 1000 - 1500 cP | |
|
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s..
|
|||
| Viscosity | 1000 - 2000 cP | 1000 - 2000 cP | |
|
Beijing Ranger Chem SM-601RX65 Solvent Based Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
|
|||
| Viscosity | 1000 cP | 1000 cP | |
|
Resinlab® CYNERGY CA6905 Adhesive