Polymer Property : Viscosity = 100000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 100000 - 200000 cP
100000 - 200000 cP
Palm Labs Adhesives Turbo Anti-Seize Copper Paste
TURBO ANTI-SEIZE – COPPER is a copper, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where prot..
Viscosity 100000 - 200000 cP
100000 - 200000 cP
Palm Labs Adhesives Turbo Anti-Seize Nickel Paste
TURBO ANTI-SEIZE – NICKEL is a gray, viscous metallic paste which may be used on all bolts, studs, value shafts, value assemblies, transmission shafts, and other types of assembly work where protec..
Viscosity 100000 cP

@Temperature 260 °C
100000 cP

@Temperature 500 °F
melt; 1500 sec-1; ISO 11443
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Viscosity 100000 cP

@Temperature 260 °C
100000 cP

@Temperature 500 °F
melt; 1500 sec-1; ISO 11443
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Viscosity 100000 - 300000 cP

@Temperature 25.0 °C
100000 - 300000 cP

@Temperature 77.0 °F
Uncured
Permabond ES558 Epoxy Resin
PERMABOND ES558 is a single-part epoxy paste which flows like solder when heated during curing. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear strength...
Viscosity 100000 cP
100000 cP
RVT, #6, 2.5 rpm; TM R050-12
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Viscosity 100000 cP
100000 cP
NextGen Adhesives G907-21 Structural Epoxy Adhesive
Description: NGAC G907-21 is a high viscosity and thixotropic adhesive system that is specifically formulated for structural bonding applications: industrial, electronics and aerospace.Advantages an..
Viscosity 100000 - 195000 cP

@Temperature 260 - 260 °C
100000 - 195000 cP

@Temperature 500 - 500 °F
Average value: 204000 cP Grade Count:9
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Viscosity 100000 - 295000 cP
100000 - 295000 cP
Average value: 233000 cP Grade Count:12
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Viscosity 100000 - 300000 cP
100000 - 300000 cP
Lord Adhesives 406 Flexible, High Impact and Peel Resistance, Medium Working Time Acrylic Adhesive
Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e..
Viscosity 100000 - 125000 cP
100000 - 125000 cP
A
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works.
Viscosity 100000 - 125000 cP
100000 - 125000 cP
A
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
Viscosity 100000 cP
100000 cP
Melt Viscosity; SABIC Method
SABIC Innovative Plastics Valox® 305 PBT
PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 1450-1850.
Viscosity 100000 cP
100000 cP
Melt Viscosity; SABIC Method
SABIC Innovative Plastics Valox® HX3061HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only.
Viscosity 100000 cP
100000 cP
Shin-Etsu Silicones KE-347TUV Silicone, RTV Coating
Information Provided by Shin-Etsu Silicones of America, Inc.
Viscosity 100000 cP
100000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
Viscosity >= 100000 cP
>= 100000 cP
mixed
Master Bond EP30-D10 Abrasion Resistant, Flexible Adhesive Compound
Description: Master Bond Polymer System EP30-D10 is a versatile two component, abrasion resistant elastomer featuring superior strength, toughness and chemical resistance for high performance bondin..
Viscosity 100000 - 150000 cP
100000 - 150000 cP
Master Bond LED401 One Component LED Curable Adhesive System
Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In..
Viscosity 100000 cP
100000 cP
mixing, dynamic
Dow Corning SILASTIC® L RTV SILICONE RUBBER BASE & CURING AGENT
Low durometer silicone mold making rubber recommended for use with rigid polyurethanes and can be used with polyesters and epoxies.Information provided by Dow Corning
Viscosity 100000 cP

@Temperature 210 °C
100000 cP

@Temperature 410 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1502E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 100000 cP

@Temperature 160 °C
100000 cP

@Temperature 320 °F
2.16 kg load; ISO 1133
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Viscosity 100000 cP
100000 cP
Cotronics 454B Machinable Non-Sag Putty Adhesive
Viscosity 100000 - 120000 cP

@Temperature 23.0 °C
100000 - 120000 cP

@Temperature 73.4 °F
Master Bond Supreme 45HTQ Quartz Filled, Heat Resistant Epoxy Compound
Master Bond Polymer Adhesive Supreme 45HTQ is a two component, toughened, quartz filled epoxy compound for high performance structural bonding and casting. It is suitable for applications where long..
Viscosity 100000 - 125000 cP
100000 - 125000 cP
A
ITW Plexus Plexus™ MA922 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works.
Viscosity 100000 - 125000 cP
100000 - 125000 cP
A
ITW Plexus Plexus™ MA925 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works.
Viscosity 100000 - 150000 cP
100000 - 150000 cP
Part A
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability
Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g..