| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
100000
cP @Temperature 260 °C |
100000
cP @Temperature 500 °F |
melt; 1500 sec-1; ISO 11443 |
|
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
|
|||
| Viscosity |
100000
cP @Temperature 260 °C |
100000
cP @Temperature 500 °F |
melt; 1500 sec-1; ISO 11443 |
|
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
|
|||
| Viscosity |
100000
cP @Temperature 260 °C |
100000
cP @Temperature 500 °F |
melt; 1500 sec-1; ISO 11443 |
|
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
|
|||
| Viscosity |
100000
-
300000
cP @Temperature 25.0 °C |
100000
-
300000
cP @Temperature 77.0 °F |
Uncured |
|
Permabond ES558 Epoxy Resin
PERMABOND ES558 is a single-part epoxy paste which flows like solder when heated during curing. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear strength...
|
|||
| Viscosity |
100000
-
195000
cP @Temperature 260 - 260 °C |
100000
-
195000
cP @Temperature 500 - 500 °F |
Average value: 204000 cP Grade Count:9 |
|
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
|
|||
| Viscosity | 100000 - 300000 cP | 100000 - 300000 cP | |
|
Lord Adhesives 204 Semi-Flexible, Medium Cure, High Viscosity Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..
|
|||
| Viscosity | 100000 - 350000 cP | 100000 - 350000 cP | |
|
Lord Adhesives 403 Flexible, High Impact and Peel Resistance, Fast Cure Acrylic Adhesive
Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e..
|
|||
| Viscosity | 100000 - 125000 cP | 100000 - 125000 cP | A |
|
ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive , high toughness.Information provided by Illinois Tool Works.
|
|||
| Viscosity | 100000 - 125000 cP | 100000 - 125000 cP | A |
|
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works.
|
|||
| Viscosity | 100000 - 125000 cP | 100000 - 125000 cP | A |
|
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works.
|
|||
| Viscosity | 100000 - 125000 cP | 100000 - 125000 cP | A |
|
ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
|
|||
| Viscosity | 100000 cP | 100000 cP | Melt Viscosity; SABIC Method |
|
SABIC Innovative Plastics Valox® 215HPR PBT
Unreinforced PBT with mold release. FDA food contact compliant in limited colors. Effective March 2008 this grade will no longer be supported with biocompatibility data. Alternative grade Valox HX21..
|
|||
| Viscosity | 100000 cP | 100000 cP | Melt Viscosity; SABIC Method |
|
SABIC Innovative Plastics Valox® 305 PBT
PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 1450-1850.
|
|||
| Viscosity | 100000 cP | 100000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
|
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
|
|||
| Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | |
|
Master Bond LED401 One Component LED Curable Adhesive System
Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In..
|
|||
| Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | |
|
Master Bond LED403Med USP Class VI, One Component, LED Curable System
Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi..
|
|||
| Viscosity |
100000
cP @Temperature 25.0 °C |
100000
cP @Temperature 77.0 °F |
After mixing |
|
Tra-Con Tra-Bond 2116 Low Vapor Pressure Epoxy Staking Compound
TRA-BOND 2116 is a thixotropic, low vapor pressure epoxy system that passes the NASA Outgassing Specification. It is recommended for critical electronic, aerospace, and industrial applications where..
|
|||
| Viscosity | >= 100000 cP | >= 100000 cP | Part B |
|
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F
Description: Master Bond Polymer System Supreme 11HT-LO is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room ..
|
|||
| Viscosity |
100000
cP @Temperature 160 °C |
100000
cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
|
EMS-Griltech Griltex® D 1539E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
|
|||
| Viscosity |
100000
-
140000
cP @Temperature 23.0 °C |
100000
-
140000
cP @Temperature 73.4 °F |
2.5 rpm |
|
Epoxy Technology EPO-TEK® OG159-2 UV Cure Optical Epoxy
Material Description: A single component, high viscosity, UV curable epoxy adhesive designed for sealing glass plates together in the LCD/OLED/display industry. It contains 1mil glass beads for bon..
|
|||
| Viscosity | 100000 - 6.00e+6 cP | 100000 - 6.00e+6 cP | |
|
3M Scotch-Weld™ 183 B/A Tan Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
|
|||
| Viscosity | 100000 cP | 100000 cP | |
|
3M Scotch-Weld™ DP5001 Structural Adhesive
Flexible and Conveyor belt repairInformation provided by 3M
|
|||
| Viscosity | 100000 cP | 100000 cP | |
|
ACC QM270 Addition Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: expanded PU foam, large obje..
|
|||
| Viscosity |
100000
-
120000
cP @Temperature 23.0 °C |
100000
-
120000
cP @Temperature 73.4 °F |
|
|
Master Bond Supreme 45HTQ Quartz Filled, Heat Resistant Epoxy Compound
Master Bond Polymer Adhesive Supreme 45HTQ is a two component, toughened, quartz filled epoxy compound for high performance structural bonding and casting. It is suitable for applications where long..
|
|||
| Viscosity | 100000 - 125000 cP | 100000 - 125000 cP | A |
|
ITW Plexus Plexus™ MA922 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works.
|
|||
| Viscosity | 100000 - 150000 cP | 100000 - 150000 cP | Part A |
|
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability
Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g..
|
|||