| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 1200 cP | 1200 cP | Part A |
|
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
|
|||
| Viscosity | 1200 cP | 1200 cP | Mixed |
|
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
|
|||
| Viscosity | 1200 cP | 1200 cP | Part A, RVT, #2, 20 rpm; TM R050-12 |
|
Resinlab® EP1112NC Clear Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Clear is a modified version of the standard EP11..
|
|||
| Viscosity | 1200 - 5000 cP | 1200 - 5000 cP | |
|
Ritelok TL22 Screwlock
Anaerobic. Low strength threadlocker for fasteners less than 1/4". Prevent corrosion, Vibration resistant, Dismantle using normal tools
|
|||
| Viscosity | 1200 - 1500 cP | 1200 - 1500 cP | Thixotropic |
|
ND Industries NutGrade® 121 Removable Threadlocker
A medium strength threadlocker. Seals most types of nuts and bolts allowing disassembly using standard tools.Typical Usesstuds and bolts, threaded pipe fittings, and locking nuts or bolts larger th..
|
|||
| Viscosity |
1200
cP @Temperature 25.0 °C |
1200
cP @Temperature 77.0 °F |
|
|
Northstar Polymers MSA-018 Isocyanate Prepolymer
Information provided by Northstar Polymers.
|
|||
| Viscosity |
1200
-
1800
cP @Temperature 25.0 °C |
1200
-
1800
cP @Temperature 77.0 °F |
Uncured |
|
Permabond 2050 Cyanoacrylate, flexible
PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding..
|
|||
| Viscosity | 1200 cP | 1200 cP | Mixed; TM R050-12 |
|
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP1112NC Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. EP1112NC Black is a modified version of the standard EP11..
|
|||
| Viscosity | 1200 cP | 1200 cP | |
|
Resinlab® TL5022 Anaerobic Threadlocking Compound
The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a ..
|
|||
| Viscosity | 1200 cP | 1200 cP | 25% Toluene Solution at 25°C; BAM 922 |
|
Kraton® D1161 K (SIS) Linear Triblock Copolymer
Description: Kraton D1161 K is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:..
|
|||
| Viscosity |
1200
cP @Shear Rate 50.0 1/s, Temperature 240 °C |
1200
cP @Shear Rate 50.0 1/s, Temperature 464 °F |
Melt; ASTM D3835 |
|
Kureha KF Polymer 850 PVDF Homopolymer
KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p..
|
|||
| Viscosity |
1200
-
1800
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200
-
1800
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2000511D1 Platinized Carbon Ink
Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working e..
|
|||
| Viscosity |
1200
cP @Temperature 25.0 °C |
1200
cP @Temperature 77.0 °F |
|
|
Struktol STRUKSILON 8010 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8010 is a specialized stabilizer for polyurethane rigid foams. Due to its extremely good nucleating performance it is especially recommended for the production of foams with a very fine c..
|
|||
| Viscosity |
1200
cP @Temperature 25.0 °C |
1200
cP @Temperature 77.0 °F |
After mixing |
|
Tra-Con Tra-Bond 2135D High Impact Epoxy Adhesive
TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact stre..
|
|||
| Viscosity |
1200
-
1500
cP @Temperature 23.9 °C |
1200
-
1500
cP @Temperature 75.0 °F |
|
|
TSE Industries EzNATE® 200 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity | 1200 - 6000 cP | 1200 - 6000 cP | Thixotropic |
|
Loctite® 242 Medium Strength Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
|
|||
| Viscosity |
1200
cP @Temperature 25.0 °C |
1200
cP @Temperature 77.0 °F |
|
|
Cytec Conathane® CE-1175 (Conap) Polyurethane Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
|
|||
| Viscosity |
1200
-
1700
cP @Temperature 23.0 °C |
1200
-
1700
cP @Temperature 73.4 °F |
100 rpm |
|
Epoxy Technology EPO-TEK® OG142-112 UV Cure Optical Epoxy
Material Description: Single component, medium viscosity, UV curable epoxy for adhesive sealing and encapsulating fiber optic and optoelectronic packaging application. Replacement version of EPO-TE..
|
|||
| Viscosity | 1200 cP | 1200 cP | Nominal |
|
Dymax Light Weld® 426 High Clarity Glass Bonding Adhesive
Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond..
|
|||
| Viscosity |
1200
-
1800
cP @Temperature 30.0 °C |
1200
-
1800
cP @Temperature 86.0 °F |
|
|
3D Systems Accura® Bluestone™ Plastic for SLA® Systems
A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the ..
|
|||
| Viscosity | 1200 cP | 1200 cP | "B" component |
|
ACC QLE 1031 QSI Quantum Silicones 25 Durometer Addition Cure Elastomer for Coating
QLE 1031 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: ..
|
|||
| Viscosity | 1200 cP | 1200 cP | B Side |
|
ACC SMP™ EP 3001 EPI Engineered Polymers Silicone Modified Polymer
EP 3001, “Powered by Reactamine® Technology”, is a two component 100% solid polyurea based sealant. EP 3001 is a self-leveling sealant designed to protect horizontal concrete. This elastomer disp..
|
|||
| Viscosity |
1200
-
1500
cP @Temperature 23.9 °C |
1200
-
1500
cP @Temperature 75.0 °F |
|
|
TSE Industries EzNATE® 200 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity | 1200 cP | 1200 cP | Part A |
|
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant
Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib..
|
|||
| Viscosity | 1200 cP | 1200 cP | |
|
Resinlab® TL5042 Anaerobic Threadlocking Compound
The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a ..
|
|||
| Viscosity |
1200
-
2200
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200
-
2200
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials D2090130P5 Pink Dielectric Ink
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||
| Viscosity |
1200
cP @Temperature 177 °C |
1200
cP @Temperature 350 °F |
Typical |
|
Bostik 6305 Good Heat Resistance EVA Glue Stick
Bostik 6305 Good Heat Resistance EVA Glue StickGood heat resistance. Adheres to a variety of coated and uncoated board stock.
|
|||
| Viscosity |
1200
cP @Temperature 25.0 °C |
1200
cP @Temperature 77.0 °F |
|
|
Zircar Zirconia ZR-CEM Zirconia Cement
Zircar Zirconia Cement Type ZR-CEM is an off white single part yttria-stabilized zirconia adhesive with a useful temperature limit of 2200°C. ZR CEM is formulated specifically for bonding Zircar Zi..
|
|||