Physical Properties Metric English Comments
Viscosity 11000 - 14000 cP
11000 - 14000 cP
Huntsman Araldite GY 2600 Bisphenol A Epoxy Liquid Resin
Weight per Epoxide (EEW, g/eq) 184 to 188. Max color is 1.Comments/Applications: High purity GY 6010 with narrow range epoxy value. Low hydrolyzable chlorine. For use in critical applications suc..
Viscosity 11000 - 14000 cP
11000 - 14000 cP
Huntsman Araldite GY 6010 Bisphenol A Epoxy Liquid Resin
Weight per Epoxide (EEW, g/eq) 182 to 192. Max color is 1.Comments/Applications: Unmodified basic liquid epoxy resin based on bis A and epichlorohydrin. General purpose, highly versatile resin for..
Viscosity 11000 - 14000 cP
11000 - 14000 cP
Huntsman Quatrex 1010 Bisphenol A Epoxy Resin
Weight per Epoxide (EEW, g/eq) 182 to 190.Comments/Applications: High purity bisphenol-A based epoxy resin.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Hun..
Viscosity 10500 - 14000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
10500 - 14000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials C2030217D2 Aluminium for PTC paste
Aluminium Ink designed to give good ohmic contact on to barium titanate PTC components. This product is particularly good where large volumes of PTC components are being processed in belt furnaces ..
Viscosity 9500 - 14000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
9500 - 14000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Gwent Electronic Materials D2080121D12 Dielectric Ink
This product is a thermoplastic screen printing ink, developed for use for flexible polymer applications. It is printed on to flexible polymeric substrates, such as Polyimide and PET substrates, to ..
Viscosity 9000 - 14000 cP

@Temperature 40.0 °C
9000 - 14000 cP

@Temperature 104 °F
Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Part A
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System
Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien..
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Part A
Master Bond EP21LVMed Two Component, Low Viscosity USP Class VI Epoxy
Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room tempera..
Viscosity 9000 - 14000 cP
9000 - 14000 cP
Part A
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System
Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick..
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Part A
Master Bond EP30-3LO Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Master Bond EP30-3LO is a two component epoxy system featuring a combination of optical clarity and light transmission, good glass transition temperature (Tg), great chemical resistance along with p..
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Part A
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System
Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi..
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Part A
Master Bond EP21CLV Two Component Epoxy System
Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a..
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Part A
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System
Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings...
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Part A
Master Bond EP42-2LV Epoxy Resists Heat and Chemicals
Description: Master Bond Polymer System EP42-2LV is a low viscosity room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring outstanding chemical resis..
Viscosity 10000 - 14000 cP

@Temperature 23.0 °C
10000 - 14000 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® 730 Unfilled Black General and Structural Grade Epoxy
Material Description: A two component, room temperature curing, general and structural grade epoxy. It can be used for adhesive, sealing, and encapsulating applications in medical, xray device, fil..
Viscosity 11000 - 14000 cP

@Temperature 23.0 °C
11000 - 14000 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® E2001-HV Electrically Conductive, Silver-Filled Epoxy
Product Description: EPO-TEK® E2001-HV Is a snap cure, two component, silver-filled die attach adhesive for semiconductor plastic IC packaging.Advantages & Application Notes:Snap cure adhesive or f..
Viscosity 11000 - 14000 cP

@Temperature 23.0 °C
11000 - 14000 cP

@Temperature 73.4 °F
20 rpm
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & ..
Viscosity 8000 - 14000 cP
8000 - 14000 cP
Accelerator
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Viscosity 8000 - 14000 cP
8000 - 14000 cP
Accelerator
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Viscosity 8000 - 14000 cP
8000 - 14000 cP
Beijing Ranger Chem 164 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 12000 - 14000 cP
12000 - 14000 cP
Aremco Aremco-Seal™ 529VHV High Temperature Specialty Coatings Silicone
Very high viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters.
Viscosity 11000 - 14000 cP
11000 - 14000 cP
50-3
Abatron AboCast 50-3/AboCure 50-1 Epoxy
Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin..
Viscosity 11000 - 14000 cP
11000 - 14000 cP
50-3
Abatron AboCast 50-3/AboCure 50-12 Epoxy
Data provided by the manufacturer, Abatron, Inc. Light motor oil viscosity, almost colorless. Shelf life is 12+ months.
Viscosity 8000 - 14000 cP
8000 - 14000 cP
Accelerator
3M Scotch-Weld™ DP420 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Viscosity 8000 - 14000 cP
8000 - 14000 cP
Accelerator
3M Scotch-Weld™ DP420 NS Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Viscosity 11000 - 14000 cP
11000 - 14000 cP
Dynamic
Dow Corning 3-0135 Cosmetic Fluid
Polydimethylsiloxane polymer with terminated, curable silanol functionality.Information provided by Dow Corning
Viscosity 8000 - 14000 cP
8000 - 14000 cP
Accelerator
3M Scotch-Weld™ DP405 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Beijing Ranger Chem HY-128 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 11000 - 14000 cP
11000 - 14000 cP
50-3
Abatron AboCast 50-3/AboCure 50-17 Epoxy
Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Dark Amber color. Shelf life is 12+ months.
Viscosity 10000 - 14000 cP
10000 - 14000 cP
Part A
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive
Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig..
Copyright © lookpolymers.com All Rights Reserved