Polymer Property : Viscosity = 175000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 175000 - 850000 cP

@Temperature 400 - 420 °C
175000 - 850000 cP

@Temperature 752 - 788 °F
Average value: 513000 cP Grade Count:11
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Viscosity 175000 cP

@Temperature 400 °C
175000 cP

@Temperature 752 °F
Melt; ISO 11443
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Viscosity 175000 - 220000 cP
175000 - 220000 cP
A
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
Viscosity 175000 - 220000 cP
175000 - 220000 cP
B
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois ..
Viscosity 175000 cP
175000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East)
VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Viscosity >= 175000 cP

@Temperature 23.0 °C
>= 175000 cP

@Temperature 73.4 °F
Master Bond EP21BAS Radiopaque Two Component Epoxy
Master Bond Polymer System EP21BAS is a radiopaque epoxy compound which offers outstanding performance and superior processability. Radiopaque epoxy polymer compounds are employed for medical diagno..
Viscosity 175000 cP

@Temperature 250 °C
175000 cP

@Temperature 482 °F
@ 1000 sec-1; ISO 11443
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Viscosity 175000 cP

@Temperature 250 °C
175000 cP

@Temperature 482 °F
@ 1000 sec-1; ISO 11443
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Viscosity 175000 - 275000 cP

@Temperature 23.0 °C
175000 - 275000 cP

@Temperature 73.4 °F
1 rpm
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive
Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p..
Viscosity 175000 cP

@Shear Rate 1000 1/s,
Temperature 280 °C
175000 cP

@Shear Rate 1000 1/s,
Temperature 536 °F
DSM Akulon® F128 PA6
Film Extrusion, Medium Viscosity
Viscosity 175000 cP
175000 cP
Melt Viscosity, 260°C, 1500 sec-1; ISO 11443
SABIC Innovative Plastics Valox® VX4920 PBT (Europe-Africa-Middle East)
VALOX VX4920 is a 20% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.