| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
1200
-
1800
cP @Temperature 30.0 °C |
1200
-
1800
cP @Temperature 86.0 °F |
|
|
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer
Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi..
|
|||
| Viscosity |
1200
-
1800
cP @Temperature 25.0 °C |
1200
-
1800
cP @Temperature 77.0 °F |
Uncured |
|
Permabond 2050 Cyanoacrylate, flexible
PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding..
|
|||
| Viscosity | 1400 - 1800 cP | 1400 - 1800 cP | 15% solution in MEK |
|
Lubrizol Advanced Materials Pearlstick® 45-90/16 Polycaprolactone based TPU
(discontinued **)
TPUs for Solvent-based adhesivesApplications: Automotive, Others, ShoeInformation provided by Merquinsa
|
|||
| Viscosity |
46.0
-
1800
cP @Temperature 52.0 - 100 °C |
46.0
-
1800
cP @Temperature 126 - 212 °F |
Average value: 717 cP Grade Count:9 |
|
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Viscosity |
150
-
1800
cP @Temperature 52.0 - 82.2 °C |
150
-
1800
cP @Temperature 126 - 180 °F |
Average value: 767 cP Grade Count:3 |
|
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
|
|||
| Viscosity | 1200 - 1800 cP | 1200 - 1800 cP | 20% Toluene Solution at 25°C; BAM 922 |
|
Kraton® G1657 M (SEBS) Linear Triblock Copolymer
Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id..
|
|||
| Viscosity | 1500 - 1800 cP | 1500 - 1800 cP | B |
|
ITW Plexus Plexusâ„¢ MA350 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low viscosity adhesive, high strength, especially suitable for battery case applications.Informati..
|
|||
| Viscosity | 600 - 1800 cP | 600 - 1800 cP | |
|
Huntsman Araldite GZ 488 N-40 US Bisphenol A Epoxy Solution
Weight per Epoxide (EEW, g/eq) 3570 to 5500. Max color is 5.Comments/Applications: Very high molecular weight solid epoxy (8,000 - 10,000), 40% solids in MEK. Outstanding adhesion, excellent flexi..
|
|||
| Viscosity |
1200
-
1800
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1200
-
1800
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2000511D1 Platinized Carbon Ink
Platinised Carbon Ink is designed to be used for screen printing working electrodes. It has been optimized to give superior electrochemical performance and designed to be used for printing working e..
|
|||
| Viscosity |
1100
-
1800
cP @Temperature 25.0 °C |
1100
-
1800
cP @Temperature 77.0 °F |
|
|
Struktol STRUKSILON 8101 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8101 is used as a silicone stabilizer for production of polyurethane rigid foam. It is especially recommended for the use in PU-1- or PU-2-component spray foam applications.Applications: ..
|
|||
| Viscosity | 1600 - 1800 cP | 1600 - 1800 cP | Part A |
|
Master Bond EP30P Epoxy Bonds Glass, Polycarbonates and Acrylics
Description: Master Bond Polymer Adhesive EP30P is a two component, transparent, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is for..
|
|||
| Viscosity |
1500
-
1800
cP @Temperature 23.0 °C |
1500
-
1800
cP @Temperature 73.4 °F |
|
|
Master Bond EP37-3FLF Low Exotherm Highly Flexible Two Component Epoxy
Master Bond Polymer System EP37-3FLF is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. The ..
|
|||
| Viscosity |
1500
-
1800
cP @Temperature 23.0 °C |
1500
-
1800
cP @Temperature 73.4 °F |
|
|
Master Bond MB297FL Cyanoacrylate Adhesive System
Vibration & shock resistant, fills gap to 0.007Information provided by Master Bond Inc.
|
|||
| Viscosity |
1600
-
1800
cP @Temperature 23.0 °C |
1600
-
1800
cP @Temperature 73.4 °F |
|
|
Master Bond EP30MED USP Class VI Certified Two Component Epoxy System
Master Bond EP30Med is a two component, optically clear, low viscosity epoxy resin system for high performance bonding, sealing, coating, and encapsulating. It features excellent physical and electr..
|
|||
| Viscosity |
1400
-
1800
cP @Temperature 23.0 °C |
1400
-
1800
cP @Temperature 73.4 °F |
|
|
Master Bond UV15-7 High Strength Non-Yellowing UV Curable System
Master Bond UV15-7 is a one component, non-yellowing UV curable polymer system for high performance bonding, sealing, coating and encapsulation. Its most salient features include superior physical s..
|
|||
| Viscosity | 1600 - 1800 cP | 1600 - 1800 cP | |
|
Epoxyset Epoxibond EB-130M-1 Unfilled Epoxy Adhesive
A two-component, non-hazmat, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc.
|
|||
| Viscosity |
1200
-
1800
cP @Temperature 30.0 °C |
1200
-
1800
cP @Temperature 86.0 °F |
|
|
3D Systems Accura® Bluestone™ Plastic for SLA® Systems
A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the ..
|
|||