| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 19000 cP | 19000 cP | |
|
Resin Technology Group 2TN Oxy-Bond™ Two-Component Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
|
|||
| Viscosity |
19000
cP @Temperature 25.0 °C |
19000
cP @Temperature 77.0 °F |
Mixed |
|
Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive
1 to1 mix ratio by volume.TIGA 108 is an epoxy adhesive system that provides excellent bond strength to most substrates. Recommended for production bonding applications, this low viscosity formulati..
|
|||
| Viscosity |
19000
cP @Temperature 25.0 °C |
19000
cP @Temperature 77.0 °F |
After mixing |
|
Tra-Con Tra-Bond 2101 General Purpose Epoxy Adhesive
TRA-BOND 2101 is a medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of its superior structural, mechanical and ele..
|
|||
| Viscosity | 19000 cP | 19000 cP | dynamic |
|
Dow Corning SE 4486 SILICONE RTV
One-part, white, moisture cure RTV, highly flowable, fast tack-free, high thermal conductivity, controlled volatility.Information provided by Dow Corning
|
|||
| Viscosity | 19000 cP | 19000 cP | Mixed |
|
Armstrong A-40 Epoxy Adhesive
Is a high viscosity, dark gray, liquid adhesive system that is qualified under Mil. Spec. MMM-A-134, Type II. NOTE: Adhesives qualified under this Specification (A-40, A-706) feature exceptional re..
|
|||
| Viscosity | 19000 cP | 19000 cP | Part B |
|
3M Scotchkote™ 323R Liquid Epoxy Coating
3M Scotchkote Rebar Liquid Patch Compound 323R is a two-part, ambient temperature cure, 100% solids content, thermosetting, liquid epoxy coating. Intended Uses:As a patch materialAs a rebar shear en..
|
|||
| Viscosity | 19000 - 24000 cP | 19000 - 24000 cP | |
|
Beijing Ranger Chem SM828S Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
|
|||
| Viscosity |
19000
cP @Temperature 177 °C |
19000
cP @Temperature 350 °F |
Typical |
|
Bostik 140 Low Cost EVA Glue Stick
Bostik 140 Low Cost EVA Glue StickLow cost. General purpose for most porous substrates used for craft / floral applications.
|
|||
| Viscosity | 19000 - 60000 cP | 19000 - 60000 cP | Thixotropic |
|
Loctite® 573 Semi-rigid Cure Anaerobic Sealant
Anaerobic GasketingLoctite® 573 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Slow curing for extended assembly operations
|
|||
| Viscosity | 19000 - 60000 cP | 19000 - 60000 cP | Thixotropic |
|
Loctite® 511 Fast Curing Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
|
|||