| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 1.00e+6 - 2.00e+6 cP @Temperature 25.0 °C |
1.00e+6 - 2.00e+6 cP @Temperature 77.0 °F |
Uncured |
| Permabond ES550 Epoxy Resin PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng.. |
|||
| Viscosity | 1.60e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
1.60e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
| Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
| Viscosity | 1.50e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
1.50e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
| Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
| Viscosity | 1.20e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
1.20e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
| Arkema Group KYNAR® 2821-00 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi.. |
|||
| Viscosity | 1.20e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
1.20e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
| Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
| Viscosity | 1.60e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
1.60e+6 - 2.00e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
| Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||