| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 200 cP | 200 cP | |
|
NextGen Adhesives G907-25 Optical Epoxy Adhesive
Description: NGAC G907-25 is a low viscosity and clear adhesive system that is specifically formulated for optical and laser applications.Advantages and Applications: The NGAC G907-25 provides high ..
|
|||
| Viscosity | 200 cP | 200 cP | |
|
Resinlab® CYNERGY CA6006 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
|
|||
| Viscosity |
200
-
300
cP @Temperature 25.0 °C |
200
-
300
cP @Temperature 77.0 °F |
Uncured |
|
Permabond UV630 UV-curable Adhesive
PERMABOND UV630 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
|
|||
| Viscosity | 200 - 375 cP | 200 - 375 cP | |
|
Huntsman AroCy B-40S Prepolymer Bisphenol-A Dicyanate
Comments/Applications: Prepolymer of high purity bisphenol A dicyanate supplied @ 75% solids in MEK. High performance multi-layer printed wiring boards and multi-chip modules.Data provided by Ciba ..
|
|||
| Viscosity | 200 - 450 cP | 200 - 450 cP | |
|
Huntsman Tactix XD 9053.03 Epoxy
Weight per Epoxide (EEW, g/eq) 160 to 210.Comments/Applications: An oligomer of Tactix 742 suitable for low pressure molding compounds.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemic..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | ASTM D803 |
|
SK Chemicals SKYTHANE® US230 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Viscosity | <= 200 cP | <= 200 cP | LV#1, 30 rpm; 540MO3C16 |
|
Solvay MIRAPOL® SURF-S 110 Surfactant
Description: Polymer to be used in acidic hard surface cleaners and delivering the following benefits through surface modification: spot free, easy cleaning, water sheeting and fast drying. pH 2 to ..
|
|||
| Viscosity | 200 cP | 200 cP | |
|
Solvay Amyl Acid Phosphate
Identification: AMYL ACID PHOSPHATE - Phosphoric acid, mono – and bis –(branched and linear pentyl esters)CAS: 84418 – 71 – 3Available in: Asia Pacific, Europe, Latin America and..
|
|||
| Viscosity | 200 - 300 cP | 200 - 300 cP | Part A |
|
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
|
|||
| Viscosity | 200 - 600 cP | 200 - 600 cP | Part A |
|
Master Bond EP30LV-1 Ultra Low Viscosity, Two Part Epoxy System
Description: Master Bond Polymer System EP30LV-1 is an ultra low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at ..
|
|||
| Viscosity |
200
-
300
cP @Temperature 23.0 °C |
200
-
300
cP @Temperature 73.4 °F |
|
|
Master Bond UV15FL One Component, High Strength, Flexible UV Curable Epoxy
Master Bond UV15FL is a one component, high strength, low viscosity, flexible UV curable epoxy resin based polymer system for bonding, sealing, & coating with exceptionally high performance properti..
|
|||
| Viscosity | 200 cP | 200 cP | Dynamic |
|
Dow Corning SYL-OFF® PMCPSL 800 Coating
Suitable for lamination with a variety of adhesives, maleate-inhibited coating offers improved thin film stability vs. conventional release coatings and excellent anchorage stability with super cale..
|
|||
| Viscosity |
200
cP @Temperature 25.0 °C |
200
cP @Temperature 77.0 °F |
|
|
Cytec (Conap) FR-1046 / EA-87 Conapoxy® Resin / Conacure® Hardener
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | |
|
Epoxyset Epoxibond EB-107LP-1 Unfilled Epoxy Adhesive
A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc.
|
|||
| Viscosity |
200
-
240
cP @Temperature 25.0 °C |
200
-
240
cP @Temperature 77.0 °F |
|
|
Esstech X-167-0000 Glass Ionomer Cement Liquid
Our GIC liquid works well when paired with an alumino-fluoro-silicate glass filler. The combination leads to a quick, easy-to-use composite material. Listed on the Toxic Substance Control Act List...
|
|||
| Viscosity |
200
cP @Temperature -35.0 °C |
200
cP @Temperature -31.0 °F |
ASTM D2983 |
|
ExxonMobil Mobil Synturion 6
Mobil Synturion 6 is a premium-quality, synthetic-base fluid specially formulated to meet the demanding lubrication and cooling requirements of mechanical seals --and to maximize seal life. The supe..
|
|||
| Viscosity | 200 cP | 200 cP | |
|
Abatron AboCast 8503-6/AboCure 8503-6 Colorless Epoxy
AboCast 8503-6/AboCure 8503-6 is a slow hardening, colorless epoxy casting compound with low viscosity used for larger castings. It allows for large castings and offers low viscosity for bubble-free..
|
|||
| Viscosity |
200
-
600
cP @Temperature 120 °C |
200
-
600
cP @Temperature 248 °F |
|
|
Abatron AboCast/AboCure 8109-1
High melting point.Processing: 100/30 pbw; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°F).Applications: Heavy duty castin..
|
|||
| Viscosity | 200 cP | 200 cP | A Side |
|
ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea
RAP-1567 HX is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generat..
|
|||
| Viscosity | 200 cP | 200 cP | Uncatalyzed, QM 230F B |
|
ACC QM 230F QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material
QM 230F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for t..
|
|||
| Viscosity | 200 cP | 200 cP | |
|
Abatron AboCast 8103-14 One-Component Epoxy
AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting..
|
|||
| Viscosity | 200 cP | 200 cP | |
|
BASF Lupranate® M20FB Isocyanate
Description: Lupranate® M20FB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20FB has faster reactivity than polymeric MDI currently used in the wood panel industry. Thi..
|
|||
| Viscosity | 200 - 500 cP | 200 - 500 cP | Mixed Viscosity |
|
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | |
|
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95%
This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo..
|
|||
| Viscosity | 200 cP | 200 cP | Part A (Isocyanate) |
|
Resinlab® UR3005 Clear Two Part Urethane Elastomer
Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi..
|
|||
| Viscosity |
200
cP @Temperature 40.0 °C |
200
cP @Temperature 104 °F |
Solution, 25% in Dimethylacetamide; Internal Method |
|
Solvay Specialty Polymers Veradel® A-704P Polyethersulfone (PESU)
(Unverified Data**)
Veradel A-704P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | 15% solution in MEK |
|
Lubrizol Advanced Materials Pearlstick® 45-40/03 Polycaprolactone based TPU
(discontinued **)
TPUs for Solvent-based adhesivesApplications: Automotive, OthersInformation provided by Merquinsa
|
|||
| Viscosity | 200 cP | 200 cP | |
|
KKPC KOSYN KSL 209 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 200 series are carboxy metamorphic styrene-butadiene latex. The KSL 200 series has good blending stability with various additives used in paper pro..
|
|||