| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 100 - 200 cP | 100 - 200 cP | |
|
ND Industries 600 Methacrylate Resin Activator
Activator for structural Adhesives and anaerobics. Solvent free.
|
|||
| Viscosity |
150
-
200
cP @Temperature 23.0 °C |
150
-
200
cP @Temperature 73.4 °F |
|
|
Prodways PLASTCure Cast 100 3D Printing Polymer
High reactivity and low viscosity. Excellent dimensional stability.Fulfills the high demands place on digital process chain.Information provided by Genistar.
|
|||
| Viscosity |
100
-
200
cP @Temperature 25.0 °C |
100
-
200
cP @Temperature 77.0 °F |
Uncured |
|
Permabond 731 Cyanoacrylate, toughened
PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
|
|||
| Viscosity |
100
-
200
cP @Temperature 25.0 °C |
100
-
200
cP @Temperature 77.0 °F |
Uncured |
|
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
|
|||
| Viscosity |
184
-
200
cP @Temperature 19.0 °C |
184
-
200
cP @Temperature 66.2 °F |
|
|
KiON CERASET® POLYSILAZANE 20 (PSZ 20)
General DescriptionKiON Ceraset Polysilazane 20 is a liquid polymer that can easily be converted to a solid pre-ceramic and then be pyrolyzed to either silicon carbide or silicon nitride-containing ..
|
|||
| Viscosity | 100 - 200 cP | 100 - 200 cP | As Supplied |
|
Heraeus Cleviosâ„¢ P T2 Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P T2 is an antistatic material based on PEDOT:..
|
|||
| Viscosity | 100 - 200 cP | 100 - 200 cP | ASTM D803 |
|
SK Chemicals SKYTHANE® US210 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Viscosity | 50 - 200 cP | 50 - 200 cP | #2 sp @ 30 rpm; RP-0596 |
|
Solvay RHODOLINE® 286N Surfactant
Description: Hydrophilic copolymer dispersant. Semi gloss to high gloss, TiO2 slurry, interior/exterior, low foam.Identification: AMMONIUM POLYACRYLATE COPOLYMER SOLUTIONAvailable in: North AmericaA..
|
|||
| Viscosity | 100 - 200 cP | 100 - 200 cP | Part B |
|
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System
Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea..
|
|||
| Viscosity |
75
-
200
cP @Temperature 125 °C |
75
-
200
cP @Temperature 257 °F |
542-111 |
|
Westlake Epolene® N-14 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-14 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
|
|||
| Viscosity | 75 - 200 cP | 75 - 200 cP | 542-111 |
|
Westlake Epolene® N-14P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Description: Epolene N-14P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
|
|||
| Viscosity | 100 - 200 cP | 100 - 200 cP | NOV QC 020 |
|
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Viscosity | 80 - 200 cP | 80 - 200 cP | dynamic |
|
Dow Corning 808 RESIN
Medium-soft, silicone resin binder for heat resistant maintenance paints and colored baking enamels.Information provided by Dow Corning
|
|||
| Viscosity |
100
-
200
cP @Temperature 23.0 °C |
100
-
200
cP @Temperature 73.4 °F |
100 rpm |
|
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy
Product Description: EPO-TEK® 301 is a two component, room temperature curing epoxy featuring very low viscosity, and excellent optical-mechanical properties.Advantages & Application Notes: Semicon..
|
|||
| Viscosity |
100
-
200
cP @Temperature 23.0 °C |
100
-
200
cP @Temperature 73.4 °F |
100 rpm |
|
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy
Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug..
|
|||
| Viscosity | 60 - 200 cP | 60 - 200 cP | |
|
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% ..
|
|||
| Viscosity | 50 - 200 cP | 50 - 200 cP | |
|
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa..
|
|||
| Viscosity | 10 - 200 cP | 10 - 200 cP | |
|
3M Scotch-Weld™ HoldFast 70 Adhesive
Extremely versatile, fast tracking industrial grade spray adhesive with unique wide-web spray pattern. Ideal for bonding a variety of substrates, including polystyrene.Features: Creates quick perman..
|
|||
| Viscosity | 50 - 200 cP | 50 - 200 cP | |
|
Beijing Ranger Chem SM-828EK85 Solvent Based Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
|
|||
| Viscosity | 10 - 200 cP | 10 - 200 cP | |
|
3M Scotch-Weld™ HoldFast 70 Cylinder Spray Adhesive
Extremely versatile, fast tracking industrial grade spray adhesive with unique wide-web spray pattern. Ideal for bonding a variety of substrates, including polystyrene.Features: Creates quick perman..
|
|||
| Viscosity | 60 - 200 cP | 60 - 200 cP | |
|
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°..
|
|||
| Viscosity | 50 - 200 cP | 50 - 200 cP | |
|
Beijing Ranger Chem SM-828X80 Solvent Based Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
|
|||