| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | |
|
ND Industries 542 Shaft & Bearing Retainer Retaining Compound
Very high strength retainer for gears, wheels, pulleys, fans, cams, collars, flywheels, rotors to shaftMeets military spec Mil-R-46082B Type III
|
|||
| Viscosity | 1600 - 2500 cP | 1600 - 2500 cP | |
|
ND Industries High Temperature SuperGlue 362
Medium viscosity with thermal cycling resistance
|
|||
| Viscosity |
2300
-
2500
cP @Temperature 23.0 °C |
2300
-
2500
cP @Temperature 73.4 °F |
|
|
Prodways PLASTCure Model 300 3D Printing Polymer
Good mechanical properties.Broad range of dental model applications.Information provided by Genistar.
|
|||
| Viscosity | 2300 - 2500 cP | 2300 - 2500 cP | Liquid State |
|
Palm Labs Adhesives Turbo Fuse Series 160SI Surface Insensitive (1000 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 180SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th..
|
|||
| Viscosity | 2300 - 2500 cP | 2300 - 2500 cP | Liquid State |
|
Palm Labs Adhesives Turbo Fuse Series 180 (2400 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 180 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
|
|||
| Viscosity | 2300 - 2500 cP | 2300 - 2500 cP | Liquid State |
|
Palm Labs Adhesives TURBO FUSE SERIES 180 BLACK TOUGHENED (2400 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 143 – BLACK TOUGHENED advanced formula is designed to polymerize instantly by absorbing surface moisture. The p..
|
|||
| Viscosity | 2300 - 2500 cP | 2300 - 2500 cP | Liquid State |
|
Palm Labs Adhesives TURBO FUSE SERIES 180 MEDICAL DEVICES APPROVED (2400 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 180 - MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moistur..
|
|||
| Viscosity |
1200
-
2500
cP @Temperature 25.0 °C |
1200
-
2500
cP @Temperature 77.0 °F |
Uncured |
|
Permabond 240 Cyanoacrylate, gap filling
PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate..
|
|||
| Viscosity | 2100 - 2500 cP | 2100 - 2500 cP | |
|
Huntsman Araldite GY 9613 Bisphenol A Epoxy Liquid Resin
Weight per Epoxide (EEW, g/eq) 188 to 197. Max color is 1.Comments/Applications: GY 2600 modified with DY 025 (Epoxide 8). Very light color. High solids and solvent free coatings and floorings.Da..
|
|||
| Viscosity | 1200 - 2500 cP | 1200 - 2500 cP | |
|
Huntsman Araldite LZ 8001 A-80 Brominated Resin
Weight per Epoxide (EEW, g/eq) 410 to 460. Max color is 2.Comments/Applications: Bis A epoxy 80% solids in acetone (18-21% bromine). For use in manufacture of thin laminates, prepregs and rigid la..
|
|||
| Viscosity |
860
-
2500
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860
-
2500
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2061027P15 High Brightness Phosphor Ink (Blue)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||
| Viscosity |
860
-
2500
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860
-
2500
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2070126D4 High Brightness Phosphor Ink (Orange)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||
| Viscosity |
860
-
2500
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860
-
2500
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2070126P5 High Brightness Phosphor Ink (White)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||
| Viscosity |
1500
-
2500
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1500
-
2500
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2070209P5 High Brightness Phosphor Ink (Green)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||
| Viscosity |
860
-
2500
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860
-
2500
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2080211P2 High Brightness Phosphor Ink (Blue/Green & Blue)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||
| Viscosity |
2100
-
2500
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
2100
-
2500
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors
This material has a high viscosity, it is a water based acrylic pressure sensitive screen printable adhesive. It can be used in many different diagnostic applications such as test cards, assays and..
|
|||
| Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | #3 SP, 12 rpm; RP-1234 |
|
Solvay MIRACARE® MS-2 Surfactant
Description: Formulated surfactant concentrate that is readily dilutable to yield ultra-mild cleansing products. Low eye and skin irritation.Chemical Name: AMPHOTERIC/ANIONIC/NONIONIC SURFACE ACTIVE..
|
|||
| Viscosity |
1000
-
2500
cP @Temperature 125 °C |
1000
-
2500
cP @Temperature 257 °F |
V-005 |
|
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h..
|
|||
| Viscosity | 300 - 2500 cP | 300 - 2500 cP | Unmilled Cement; Zeon Test #328 |
|
Zeon Chemicals HyTemp® 4051CG AR Polyacrylate Elastomer
HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Cement grade version of Hy..
|
|||
| Viscosity | 500 - 2500 cP | 500 - 2500 cP | Milled Cement; Zeon Test #327 |
|
Zeon Chemicals Nipol® 1031 Nitrile Elastomer
Nipol 1031 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent fuel a..
|
|||
| Viscosity | 1800 - 2500 cP | 1800 - 2500 cP | Part A |
|
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin
Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used..
|
|||
| Viscosity |
2100
-
2500
cP @Temperature 23.0 °C |
2100
-
2500
cP @Temperature 73.4 °F |
|
|
Master Bond EP27 Low Temperature Curing Two Component Epoxy
Master Bond Polymer System EP27 is a unique two component
epoxy formulation offers relatively fast cures at temperatures as low as 40°F and below, with curing times much shorter than currently exis..
|
|||
| Viscosity |
1500
-
2500
cP @Temperature 23.0 °C |
1500
-
2500
cP @Temperature 73.4 °F |
|
|
Master Bond UV15-7DC One Component, Dual Cure UV System
Master Bond UV15-7DC is a one component, dual cure UV system for high performance bonding, sealing, coating and encapsulation applications. This system features a primary cure utilizing UV light and..
|
|||
| Viscosity | 300 - 2500 cP | 300 - 2500 cP | Solution 15% in MEK |
|
Wanhua Chemical Wanthane® WHT-65 TPU Solvent-Based Adhesive
Wide viscosity range, high crystallization rate, low activation temperature, good solvent solubility, accurate control of viscosity, outstanding bonding strength for PVC, polyamide, polyester, PU, c..
|
|||
| Viscosity | 1000 - 2500 cP | 1000 - 2500 cP | |
|
Abatron AboCast/AboCure 8109-6
High heat resistance. Easy to use.Processing: 100/90 pbw; Potlife: 15-20 days/20°C (68°F), 7-10 h/120°C (250°F); mix at RT; cures in: 3 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applicat..
|
|||
| Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | MA143LFE |
|
C.O.I.M. FILCO® 309 Film Former for Glass Fiber Sizes
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar..
|
|||
| Viscosity |
500
-
2500
cP @Temperature 25.0 °C |
500
-
2500
cP @Temperature 77.0 °F |
spindle n 3-10 RPM; MA143LFE |
|
C.O.I.M. FILCO® 650 Film Former for Glass Fiber Sizes
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar..
|
|||
| Viscosity |
1500
-
2500
cP @Temperature 35.0 °C |
1500
-
2500
cP @Temperature 95.0 °F |
|
|
C.O.I.M. UREXTER® T 404 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
|
|||
| Viscosity | 2000 - 2500 cP | 2000 - 2500 cP | Brooksfield LV Viscometer |
|
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
|
|||
| Viscosity | 2000 - 2500 cP | 2000 - 2500 cP | Brooksfield LV Viscometer |
|
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating
Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available.
|
|||