| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
275000
-
275000
cP @Temperature 260 - 260 °C |
275000
-
275000
cP @Temperature 500 - 500 °F |
Average value: 229000 cP Grade Count:1 |
|
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
|
|||
| Viscosity |
275000
-
275000
cP @Shear Rate 1000 - 1000 1/s |
275000
-
275000
cP @Shear Rate 1000 - 1000 1/s |
Average value: 229000 cP Grade Count:1 |
|
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
|
|||
| Viscosity |
175000
-
275000
cP @Temperature 23.0 °C |
175000
-
275000
cP @Temperature 73.4 °F |
1 rpm |
|
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive
Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p..
|
|||
| Viscosity | 150000 - 275000 cP | 150000 - 275000 cP | Base |
|
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
|
|||