| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 280 - 320 cP | 280 - 320 cP | Liquid State |
|
Palm Labs Adhesives TURBO FUSE SERIES 143 BLACK TOUGHENED (300 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 143 – BLACK TOUGHENED advanced formula is designed to polymerize instantly by absorbing surface moisture. The p..
|
|||
| Viscosity | 280 - 400 cP | 280 - 400 cP | 25% Toluene Solution at 25°C; BAM 922 |
|
Kraton® D1124 P (SIS) Branched Copolymer
Description: Kraton D1124 P is a clear, branched copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: Kraton ..
|
|||
| Viscosity | 280 - 500 cP | 280 - 500 cP | Part B |
|
Master Bond EP30ANHT Two Part, Electrically Isolating Epoxy Adhesive
Description: Master Bond Polymer System EP30ANHT is a two part epoxy system with terrific thermal conductivity, while maintaining electrical insulation. One noteworthy property is its wide service t..
|
|||
| Viscosity | 280 - 500 cP | 280 - 500 cP | Part B |
|
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy
Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi..
|
|||
| Viscosity | 280 - 500 cP | 280 - 500 cP | Part B |
|
Master Bond EP30LV-1 Ultra Low Viscosity, Two Part Epoxy System
Description: Master Bond Polymer System EP30LV-1 is an ultra low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at ..
|
|||
| Viscosity | 280 cP | 280 cP | Extrusion measured at 50 psi/0.125" orifice. |
|
Loctite® Output™ 5404 Heat Cure Silicone
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
|
|||