| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 300 cP | 300 cP | |
|
Resinlab® CYNERGY CA6401 Adhesive
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
|
|||
| Viscosity | 300 cP | 300 cP | Approximately |
|
Abatron KromaKote 8901-8 Polyurethane Coating
(discontinued **)
2-component system for outstanding performance in normal, industrial, marine and corrosive environments. Superb combination of chemical, solvent, abrasion and weather resistance.Suggested Uses: Pro..
|
|||
| Viscosity |
300
-
900
cP @Temperature 25.0 °C |
300
-
900
cP @Temperature 77.0 °F |
|
|
Northstar Polymers CPB-046 Polyether Curing Agent
Information provided by Northstar Polymers.
|
|||
| Viscosity |
300
-
500
cP @Temperature 25.0 °C |
300
-
500
cP @Temperature 77.0 °F |
Mixed |
|
Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System
Mix ratio 2 to 1 by volume.UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy bas..
|
|||
| Viscosity | 300 cP | 300 cP | Fed Std Method 4287 |
|
Humiseal 1C61 UV Cure Conformal Coating
Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t..
|
|||
| Viscosity | 300 - 800 cP | 300 - 800 cP | |
|
Huntsman AroCy M-20 Monomeric Bisphenol F Dicyanate
Comments/Applications: Low melt viscosity coprepolymer of M-30/B-30 type materials. RTM, unidirectional prepreg manufacture for radomes, high gain antennas and high density circuitry.Data provided ..
|
|||
| Viscosity |
300
cP @Temperature 30.0 °C |
300
cP @Temperature 86.0 °F |
5% wt Toluene Solution |
|
Kuraray SEPTON® S4077 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
|
|||
| Viscosity | <= 300 cP | <= 300 cP | |
|
Solvay Specialty Polymers Solvera® PT 5060 PFPE Surface Treatment
Solvera® PFPE is a sustainable surface treatment developed to increase the grease resistance of paper packaging, pizza boxes, popcorn bags, pet food bags and food wraps. Both solvent and aqueous..
|
|||
| Viscosity |
<=
300
cP @Temperature 176 °C |
<=
300
cP @Temperature 349 °F |
|
|
Solvay REPEL-O-TEX® SRP-6 Polyethylene Glycol Polyester
Description: Soil Release Polymer offering protection against the adhesion of greasy soils between two wash cycles. 100% active material in powder form.Chemical Name: POLYETHYLENE GLYCOL POLYESTERCA..
|
|||
| Viscosity |
300
-
400
cP @Temperature 125 °C |
300
-
400
cP @Temperature 257 °F |
TXAL-A-XX-G-V-005 |
|
Westlake Epolene® E-14P Oxidized Low Molecular Weight Polyethylene Polymer
Description: The Epolene E-14P is a low molecular-weight, low-density, oxidized polyethylene powder. It is useful as a lubricant in processing rigid and flexible polyvinyl chloride (PVC) and as a pr..
|
|||
| Viscosity | 300 - 2700 cP | 300 - 2700 cP | Unmilled Cement; Zeon Test #328 |
|
Zeon Chemicals HyTemp® 4051CG Polyacrylate Curative
HyTemp 4451CG is a ground form of HyTemp 4051CG, which contains one or more acrylic esters with a small percentage of a carboxy/chlorine cure site.Contains acrylic esters with a small percentage of ..
|
|||
| Viscosity |
300
cP @Temperature 25.0 °C |
300
cP @Temperature 77.0 °F |
Mixed (sp #4, 30 rpm) |
|
Tra-Con Tra-Bond FS469 Clear High Strength Epoxy
TRA-BOND FS469 is a clear low viscosity epoxy formulation designed for bonding and coating micro-electronics, laminations, optical components and laser assemblies. The low cure shrinkage (using a ro..
|
|||
| Viscosity | 300 - 400 cP | 300 - 400 cP | Part B |
|
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
|
|||
| Viscosity |
300
cP @Temperature 200 °C |
300
cP @Temperature 392 °F |
Melt |
|
Unitika elitel UE3216 Polyester, Pellet
Low Tg type UE3215UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders, and modi..
|
|||
| Viscosity | 300 - 700 cP | 300 - 700 cP | NOV QC 020 |
|
Lubrizol ESTANE® 5701F1 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Viscosity | 300 cP | 300 cP | Dynamic |
|
Dow Corning SYL-OFF® PMCPSL 3000 Catalyst
1,000 ppm platinum in vinyl polymerInformation provided by Dow Corning
|
|||
| Viscosity | 300 cP | 300 cP | |
|
Elmer's Products Aron Alpha® 432TB Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
|
|||
| Viscosity |
300
-
600
cP @Temperature 23.0 °C |
300
-
600
cP @Temperature 73.4 °F |
100 rpm |
|
Epoxy Technology EPO-TEK® OG178 UV Cure Optical Epoxy
Material Description: A single component, UV/visible shifted light curable epoxy, designed for adhesive, sealing, coating and encapsulating applications found in semiconductor, electro-optics, fiber..
|
|||
| Viscosity | 300 - 600 cP | 300 - 600 cP | |
|
Epoxyset Epoxibond EB-107LP-2 Unfilled Epoxy Adhesive
A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc.
|
|||
| Viscosity | 300 - 500 cP | 300 - 500 cP | |
|
C.O.I.M. FILCO® 300 Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber Sizing
Description: Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in..
|
|||
| Viscosity | 300 cP | 300 cP | |
|
Atom Adhesives AA-BOND 2113 Epoxy Adhesive
AA-BOND 2113 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flow ability and wetting characteristics, and adheres strongly to gla..
|
|||
| Viscosity | 300 - 500 cP | 300 - 500 cP | |
|
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
| Viscosity | 300 - 500 cP | 300 - 500 cP | |
|
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Viscosity | 300 - 400 cP | 300 - 400 cP | |
|
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone
Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC)
|
|||
| Viscosity | 300 - 600 cP | 300 - 600 cP | Mixed Viscosity |
|
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..
|
|||
| Viscosity | 300 cP | 300 cP | Part B, RVT, #3, 2.5 rpm; TM R050-12 |
|
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin
Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate ..
|
|||
| Viscosity | 300 - 800 cP | 300 - 800 cP | LV# @ 60 rpm; RP-0596 |
|
Solvay RHODOLINE® 670 Surfactant
Description: Highly effective mineral oil defoamer for latex processing..Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE 670 is an APE-free and silicone–free def..
|
|||
| Viscosity | 300 cP | 300 cP | |
|
KKPC KOSYN KSL 207 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 200 series are carboxy metamorphic styrene-butadiene latex. The KSL 200 series has good blending stability with various additives used in paper pro..
|
|||