| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
100
-
300
cP @Temperature 32.2 °C |
100
-
300
cP @Temperature 90.0 °F |
|
|
Old Hickory UltraCast Slurry PC-2000 Kentucky Ball Clay
These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c..
|
|||
| Viscosity |
100
-
300
cP @Temperature 32.2 °C |
100
-
300
cP @Temperature 90.0 °F |
|
|
Old Hickory UltraCast Slurry UC-34A Kentucky Ball Clay
These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c..
|
|||
| Viscosity |
150
-
300
cP @Temperature 25.0 °C |
150
-
300
cP @Temperature 77.0 °F |
Uncured |
|
Permabond HL138 Anaerobic Retaining Compound
Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which ..
|
|||
| Viscosity |
100
-
300
cP @Temperature 32.2 °C |
100
-
300
cP @Temperature 90.0 °F |
|
|
Old Hickory UltraCast Slurry PC-2034 Kentucky Ball Clay
These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c..
|
|||
| Viscosity |
200
-
300
cP @Temperature 25.0 °C |
200
-
300
cP @Temperature 77.0 °F |
Uncured |
|
Permabond UV630 UV-curable Adhesive
PERMABOND UV630 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon..
|
|||
| Viscosity | 150 - 300 cP | 150 - 300 cP | |
|
Huntsman HY 847 Cycloaliphatic Amine
Approx. H+ equivalent weight 75. Mix Ratio with GY 6010 is 40.Comments/Applications: Medium viscosity, high performance hardener for self-leveling flooring.Data provided by Ciba Specialty Chemical..
|
|||
| Viscosity | 101 - 300 cP | 101 - 300 cP | ASTM D445 |
|
IRPC Polimaxx Polene PE250N Polypropylene Wax
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
|
|||
| Viscosity |
5.0
-
300
cP @Temperature 20.0 °C |
5.0
-
300
cP @Temperature 68.0 °F |
2%, Hoppler |
|
Mikro-Technik 8036 R/U Carboxymethylcellulose (CMC)
Purified GradeComments: All grades are available neutralized with carbon dioxide (no suffix or suffix K) or acetic acid (suffix E). Reduced active contents down to 50 % are available. Special conce..
|
|||
| Viscosity |
150
-
300
cP @Temperature 125 °C |
150
-
300
cP @Temperature 257 °F |
TXAL-A-XX-G-V-005 |
|
Westlake Epolene® E-14E Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Product Description: The Epolene E-14E is a low molecular weight, low density, oxidized polyethylene. The low molecular weight and low softening point contribute to the production of stable, low col..
|
|||
| Viscosity |
150
-
300
cP @Temperature 125 °C |
150
-
300
cP @Temperature 257 °F |
TXAL-A-XX-G-V-005 |
|
Westlake Epolene® E-14EP Oxidized Low Molecular Weight Polyethylene Polymer
Description: The Epolene E-14EP is a low molecular weight, low density, oxidized polyethylene powder. The low molecular weight and low softening point contribute to the production of stable, low col..
|
|||
| Viscosity | 200 - 300 cP | 200 - 300 cP | Part A |
|
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
|
|||
| Viscosity |
200
-
300
cP @Temperature 23.0 °C |
200
-
300
cP @Temperature 73.4 °F |
|
|
Master Bond UV15FL One Component, High Strength, Flexible UV Curable Epoxy
Master Bond UV15FL is a one component, high strength, low viscosity, flexible UV curable epoxy resin based polymer system for bonding, sealing, & coating with exceptionally high performance properti..
|
|||
| Viscosity |
100
-
300
cP @Temperature 75.0 °C |
100
-
300
cP @Temperature 167 °F |
|
|
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity |
150
-
300
cP @Temperature 23.0 °C |
150
-
300
cP @Temperature 73.4 °F |
100 rpm |
|
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy
Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:..
|
|||
| Viscosity |
100
-
300
cP @Temperature 23.0 °C |
100
-
300
cP @Temperature 73.4 °F |
100 rpm |
|
Epoxy Technology EPO-TEK® MA-5 Optical Grade Epoxy
Material Description: A single component, B-stageable, optical grade epoxy for fiber optic assembly. It may be used for B-stage sealing of fiber cables into ferrules, or fiber optic feed through in..
|
|||
| Viscosity |
250
-
300
cP @Temperature 30.0 °C |
250
-
300
cP @Temperature 86.0 °F |
|
|
3D Systems Accura® Xtreme Plastic for SLA® Systems
For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte..
|
|||
| Viscosity |
150
-
300
cP @Temperature 25.0 °C |
150
-
300
cP @Temperature 77.0 °F |
|
|
BorsodChem ONGRONAT PE-210 MDI Isocyanate
Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyester-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for ..
|
|||
| Viscosity | 50 - 300 cP | 50 - 300 cP | RP-0596 |
|
Solvay RHODAPON® SB-8208/S STD Surfactant
Description: Rhodapon® LX-28/AF3 is Sodium Lauryl Sulfate solution based on narrow-cut primary natural alcohol. This grade is preserved with Formalin. It provides excellent detergency, cleansing an..
|
|||
| Viscosity | 100 - 300 cP | 100 - 300 cP | #2 sp @ 30 rpm; RP-0596 |
|
Solvay RHODOLINE® 270 Surfactant
Description: Polyacid dispersant. Highly versatile, economical and low foam, flat to gloss, ideal for interior application.Identification: ACRYLIC POLYMERCAS: 9003-04-7Available in: North America IR..
|
|||
| Viscosity |
100
-
300
cP @Temperature 75.0 °C |
100
-
300
cP @Temperature 167 °F |
|
|
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||