Polymer Property : Viscosity = 3000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 1600 - 3000 cP
1600 - 3000 cP
Thixotropic
ND Industries StudGrade® 131 Permanent CT Threadlocker
General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m..
Viscosity 2000 - 3000 cP

@Temperature 25.0 °C
2000 - 3000 cP

@Temperature 77.0 °F
Uncured
Permabond UV620 UV-curable Adhesive
PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I..
Viscosity 2000 - 3000 cP
2000 - 3000 cP
Huntsman Araldite GY 285 Bisphenol F Epoxy Resin
Weight per Epoxide (EEW, g/eq) 163 to 172. Max color is 5.Comments/Applications: Used in coatings, adhesives, tank linings, flooring, filament winding, casting pultrusion and RTM. Better chemical ..
Viscosity 2000 - 3000 cP
2000 - 3000 cP
25% Toluene Solution at 25°C; KM 06
Kraton® D1116 A (SBS) Radial Triblock Copolymer
Description: Kraton D1116 A is a clear, radial triblock copolymer based on styrene and butadiene with a polystyrene content of 23%. It is supplied from Europe in the physical form identified: Kraton..
Viscosity 2000 - 3000 cP
2000 - 3000 cP
25% Toluene Solution at 25°C; KM 06
Kraton® D1116 E (SBS) Radial Triblock Copolymer
Description: Kraton D1116 E is a clear, radial triblock copolymer based on styrene and butadiene with a polystyrene content of 23%. It is supplied from Europe in the physical form identified: Kraton..
Viscosity 1500 - 3000 cP
1500 - 3000 cP
Lucite International Colacryl ® 1205 Acrylic Solution Resin
Butyl Methacrylate polymers are more flexible and softer than Methyl Methacrylate types. The polymers are compatible with nitrocellulose, chlorinated rubber, some phenolics and maleics. Butyl methac..
Viscosity 2000 - 3000 cP
2000 - 3000 cP
20% Toluene Solution at 25°C; BAM 922
Kraton® D1116 K (SBS) Radial Triblock Copolymer
Description: Kraton D1116 K is a clear, radial triblock copolymer based on styrene and butadiene, with a polystyrene content of 23%. It is supplied from North America in the physical form identified..
Viscosity 2500 - 3000 cP
2500 - 3000 cP
As Supplied
Heraeus Cleviosâ„¢ S V3 Antistatic/Conductive Polymer Coating for Screen Printing
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as a paste designed for application by silk screen printing to be used for transparent conductive devices. Cleviosâ„¢ S V3 grade ..
Viscosity 1500 - 3000 cP
1500 - 3000 cP
Part A
Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating
Product Description: Master Bond EP21LVSP6 is a two component epoxy compound for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at room temperature or more ra..
Viscosity 2000 - 3000 cP

@Temperature 23.0 °C
2000 - 3000 cP

@Temperature 73.4 °F
Master Bond EP39-2 Fast Curing Optically Clear Two Component Epoxy System
Master Bond Polymer System EP39-2 is a fast curing, low viscosity, optically clear two component epoxy system for high performance bonding, sealing, coating and casting. It is 100% reactive and does..
Viscosity 2000 - 3000 cP

@Temperature 23.0 °C
2000 - 3000 cP

@Temperature 73.4 °F
Master Bond EP30M3LV Electrically Insulative, Low Viscosity Two Component Epoxy
Master Bond Polymer System EP30M3LV is a lower viscosity, two component epoxy system for high performance bonding, sealing and encapsulation. It is formulated to cure at ambient temperatures or mor..
Viscosity 2000 - 3000 cP

@Temperature 23.0 °C
2000 - 3000 cP

@Temperature 73.4 °F
Master Bond EP31 High Shear and Peel Strength Room Temperature Curing Epoxy
Master Bond Polymer System EP31 is a two component room temperature curing epoxy for high performance structural bonding applications featuring lap shear strengths exceeding 4600 psi. In addition, u..
Viscosity 1000 - 3000 cP
1000 - 3000 cP
Solution 15% in MEK
Wanhua Chemical Wanthane® WHT-6420B TPU Solvent-Based Adhesive
Wide viscosity range, high crystallization rate, low activation temperature, good solvent solubility, accurate control of viscosity, outstanding bonding strength for PVC, polyamide, polyester, PU, c..
Viscosity 1000 - 3000 cP

@Temperature 23.0 °C
1000 - 3000 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy
Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
Viscosity 1500 - 3000 cP

@Temperature 23.0 °C
1500 - 3000 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® 320NC-2 Optically Opaque Epoxy
Material Description: A two component, black colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific..
Viscosity 1000 - 3000 cP
1000 - 3000 cP
dynamic
Dow Corning 2-2078 FLUID
A liquid amino phenyl silicone resin primarily for use in hair care products, but has utility in color cosmetics as well.Information provided by Dow Corning
Viscosity 500 - 3000 cP

@Temperature 25.0 °C
500 - 3000 cP

@Temperature 77.0 °F
spindle n 3-10 RPM; MA143LFE
C.O.I.M. FILCO® 362 Film Former for Glass Fiber Sizes
Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar..
Viscosity 2500 - 3000 cP

@Temperature 35.0 °C
2500 - 3000 cP

@Temperature 95.0 °F
Dynamic viscosity
C.O.I.M. PLAXTER® P 80 Low Viscosity Polymeric Plasticizer
Description: Formulated with PVC, it is used in in the production of stretch film for food contact.Information provided by P.A.T. Products, Inc.
Viscosity 2000 - 3000 cP

@Temperature 35.0 °C
2000 - 3000 cP

@Temperature 95.0 °F
C.O.I.M. UREXTER® F 3 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
Viscosity 2000 - 3000 cP

@Temperature 35.0 °C
2000 - 3000 cP

@Temperature 95.0 °F
C.O.I.M. UREXTER® Lp 2500_30 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
Viscosity 2000 - 3000 cP

@Temperature 35.0 °C
2000 - 3000 cP

@Temperature 95.0 °F
C.O.I.M. UREXTER® Lp 285 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
Viscosity 2000 - 3000 cP
2000 - 3000 cP
3M Pronto™ CA-5 Instant Adhesive
One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A high viscosity, slower settin..
Viscosity 2000 - 3000 cP
2000 - 3000 cP
mixed
Master Bond EP39MHT Two Component, Room Temperature Curing Epoxy Resin System
Master Bond Polymer System EP39MHT is a low viscosity, two component, epoxy resin system for high performance potting, encapsulation, sealing and bonding. It cures readily at ambient temperatures to..
Viscosity 500 - 3000 cP

@Shear Rate 1.00e+10 1/s,
Temperature 20.0 °C
500 - 3000 cP

@Shear Rate 1.00e+10 1/s,
Temperature 68.0 °F
Kraton® NEXAR™ MD9150 Polymer Barrier Membrane Solution
NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification and d..
Viscosity 1500 - 3000 cP
1500 - 3000 cP
Part B
Master Bond EP33LV Epoxy Has Dimensional Stability and Machinability
Description: Master Bond EP33LV is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g..
Viscosity 1500 - 3000 cP

@Temperature 35.0 - 35.0 °C
1500 - 3000 cP

@Temperature 95.0 - 95.0 °F
Average value: 2380 cP Grade Count:5
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced