Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 300000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 300000 cP
300000 cP
NextGen Adhesives P907-30 Optical Assembly Adhesive
Description: NGAC P907-30 is a high viscosity, controlled flow encapsulant designed for microelectronics applications requiring low shrinkage and high reliability performance.Advantages and Applicat..
Viscosity 300000 cP

@Temperature 400 °C
300000 cP

@Temperature 752 °F
melt; ISO 11443
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Viscosity 300000 cP

@Temperature 400 °C
300000 cP

@Temperature 752 °F
melt; ISO 11443
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
Viscosity 300000 - 1.90e+6 cP

@Temperature 190 - 190 °C
300000 - 1.90e+6 cP

@Temperature 374 - 374 °F
Average value: 495000 cP Grade Count:22
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
Viscosity 300000 cP
300000 cP
Part B, Spindle TD, 2.5 rpm; Uncured
Resinlab® AR 4305 HP Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 HP is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 HP forms tough, dur..
Viscosity 300000 cP
300000 cP
Part A, Spindle TD, 2.5 rpm; Uncured
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive
Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any ..
Viscosity 300000 - 1.00e+6 cP
300000 - 1.00e+6 cP
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Viscosity 300000 - 400000 cP
300000 - 400000 cP
Paste
Lucas-Milhaupt Lucanex 716 Active Metal Brazing
Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste
Viscosity 300000 - 400000 cP
300000 - 400000 cP
Paste
Lucas-Milhaupt Lucanex 721 Active Metal Brazing
Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste
Viscosity 300000 cP

@Temperature 25.0 °C
300000 cP

@Temperature 77.0 °F
Dynamic
Struktol POLYDIS 3691 Elastomer modified epoxy prepolymer
Applications: STRUKTOL POLYDIS 3691 is used where conventional epoxy systems are unable to satisfy the demands of for example contact adhesion or peel strength. Improvements in impact strength, flex..
Viscosity 300000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
300000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 1124 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 260 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 500 °F
melt viscosity; b.o. ISO 11443-A
Covestro Bayblend® T65 HI PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature ..
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 240 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 464 °F
DSM Akulon® F127 PA6
Low/Medium Viscosity, Film Extrusion
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 280 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 536 °F
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 280 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 536 °F
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 240 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 464 °F
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 260 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 500 °F
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 280 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 536 °F
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 240 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 464 °F
DSM Akulon® XP32-E1 PA6
Film Extrusion, Medium Viscosity, Lubricated, Nucleated
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 240 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 464 °F
DSM Akulon® XP36-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 240 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 464 °F
DSM Akulon® XP32-C1 PA6
Film Extrusion, Medium Viscosity, Lubricated
Viscosity 300000 cP

@Shear Rate 1000 1/s,
Temperature 240 °C
300000 cP

@Shear Rate 1000 1/s,
Temperature 464 °F
DSM Akulon® XP36-E1 PA6
Film Extrusion, Medium Viscosity, Nucleated, Lubricated
Viscosity 300000 - 1.00e+6 cP
300000 - 1.00e+6 cP
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
Viscosity 300000 - 800000 cP
300000 - 800000 cP
Part B
Master Bond EP21TDC-2LO Two component, highly flexibilized epoxy resin compound
Product Description: Master Bond Polymer System EP21TDC-2LO is a two component, highly flexible epoxy resin compound for high performance bonding, sealing, coating, and encapsulation. It is formulat..
Viscosity 300000 cP
300000 cP
Part B, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..
Viscosity 300000 cP
300000 cP
Part B, RVT, #7, 2.5 rpm; TM R050-12
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go..
Viscosity 300000 cP

@Temperature 400 °C
300000 cP

@Temperature 752 °F
melt; ISO 11443
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
Copyright © lookpolymers.com All Rights Reserved