| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 300000 cP | 300000 cP | |
|
NextGen Adhesives P907-30 Optical Assembly Adhesive
Description: NGAC P907-30 is a high viscosity, controlled flow encapsulant designed for microelectronics applications requiring low shrinkage and high reliability performance.Advantages and Applicat..
|
|||
| Viscosity |
300000
cP @Shear Rate 190 1/s, Temperature 230 °C |
300000
cP @Shear Rate 190 1/s, Temperature 446 °F |
|
|
Noltex Soarnol® BG3522 Ethylene Vinyl Alcohol Copolymer
Special designed high MFI grade. New EVOH for extrusion coating. Ethylene content 35 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, ..
|
|||
| Viscosity |
300000
cP @Temperature 400 °C |
300000
cP @Temperature 752 °F |
melt; ISO 11443 |
|
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
|
|||
| Viscosity |
300000
-
1.90e+6
cP @Shear Rate 50.0 - 50.0 1/s |
300000
-
1.90e+6
cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 495000 cP Grade Count:22 |
|
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
|
|||
| Viscosity | 300000 cP | 300000 cP | Part B, Spindle TD, 2.5 rpm; Uncured |
|
Resinlab® AR 4400 Metal & Composite Bonding Methacrylate Adhesive
Resinlab™ AR 4400 is a 1:1 mix methacrylate-based structural adhesive formulated to bond almost all engineered thermoplastics, thermosets, composites, and metal structural elements together in any ..
|
|||
| Viscosity | 300000 - 1.00e+6 cP | 300000 - 1.00e+6 cP | |
|
Lord Adhesives 320 Toughened, High Viscosity SMC, FRP, General Purpose Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
|
|||
| Viscosity | 300000 - 400000 cP | 300000 - 400000 cP | Paste |
|
Lucas-Milhaupt Lucanex 716 Active Metal Brazing
Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste
|
|||
| Viscosity |
300000
cP @Shear Rate 50.0 1/s, Temperature 190 °C |
300000
cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
|
DuPont Bynel® 1124 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
|
|||
| Viscosity | 300000 - 500000 cP | 300000 - 500000 cP | Dynamic |
|
Dow Corning 9041 Silicone Elastomer Blend
A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, haircare, color cosmetics, suncare, antiperspirants and deodorants, and w..
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
|
Covestro Bayblend® T65 HI PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Improve low temperature ..
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F127 PA6
Low/Medium Viscosity, Film Extrusion
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
|
DSM Akulon® F130-C PA6
Film Extrusion, Medium Viscosity, Lubricated
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
|
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
|
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
|
DSM Akulon® F132-C1 PA6
Film Extrusion, High Viscosity, Lubricated
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
|
DSM Akulon® F132-E2 PA6
High Viscosity, Nucleated, Lubricated, Film Extrusion
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 280 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 536 °F |
|
|
DSM Akulon® F234-C PA6
Film Extrusion, High Viscosity, Lubricated
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® XP32-E1 PA6
Film Extrusion, Medium Viscosity, Lubricated, Nucleated
|
|||
| Viscosity | 300000 - 400000 cP | 300000 - 400000 cP | 1 rpm |
|
Epoxy Technology EPO-TEK® 430 Epoxy
Product Description: A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding ..
|
|||
| Viscosity |
300000
cP @Shear Rate 1000 1/s, Temperature 240 °C |
300000
cP @Shear Rate 1000 1/s, Temperature 464 °F |
|
|
DSM Akulon® XP36-E1 PA6
Film Extrusion, Medium Viscosity, Nucleated, Lubricated
|
|||
| Viscosity | 300000 - 1.00e+6 cP | 300000 - 1.00e+6 cP | |
|
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
|
|||
| Viscosity | 300000 cP | 300000 cP | Part B, RVT, #7, 2.5 rpm; TM R050-12 |
|
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go..
|
|||
| Viscosity |
300000
cP @Temperature 400 °C |
300000
cP @Temperature 752 °F |
melt; ISO 11443 |
|
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
|
|||