| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 250 - 350 cP | 250 - 350 cP | |
|
ND Industries 333 Surface Insensitive Instant Superglue
Low-medium viscosity for difficult to bond substrates
|
|||
| Viscosity | 250 - 350 cP | 250 - 350 cP | |
|
ND Industries SuperGlue Ethyl 300
General DescriptionA medium to low viscosity cyanoacrylate which is used for bonding plastics and rubber in various combinations.Meets military spec Mil-A-46050C Type II Class II
|
|||
| Viscosity |
250
-
350
cP @Temperature 82.2 °C |
250
-
350
cP @Temperature 180 °F |
|
|
Northstar Polymers SBA-036 Polyester Curing Agent
Information provided by Northstar Polymers.
|
|||
| Viscosity |
250
-
350
cP @Temperature 82.2 °C |
250
-
350
cP @Temperature 180 °F |
|
|
Northstar Polymers SBA-041 Polyester Curing Agent
Information provided by Northstar Polymers.
|
|||
| Viscosity | 50 - 350 cP | 50 - 350 cP | |
|
Huntsman HY 5200 Aromatic Amine
Approx. H+ equivalent weight 45. Mix Ratio with GY 6010 is 23.Comments/Applications: Liquid aromatic amine.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by H..
|
|||
| Viscosity | 210 - 350 cP | 210 - 350 cP | |
|
Solvay IGEPAL® CO 710 Surfactant
Chemical Name: NONYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHEDCAS: 68412-54-4 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CO-710 is an excellent prima..
|
|||
| Viscosity | 50 - 350 cP | 50 - 350 cP | #2 SP at 60 rpm; 540MA3C56 |
|
Solvay MIRAPOL® SURF-S 480PF Surfactant
Description: Rinse aid polymer specially formulated for auto dish wash powders, tablets and liquids. Phosphate-free. Recommended as a substitute to rinse aid surfactants. Enables raw material cost s..
|
|||
| Viscosity | 250 - 350 cP | 250 - 350 cP | |
|
Dow CYRACURE™ UVR-6107 Cycloaliphatic Epoxide
CYRACURE™ UVR-6107 cycloaliphatic epoxide is a low viscosity base resin. Typical applications include: Metal decoration coatings Overprint varnishes Information provided by Dow
|
|||
| Viscosity | 250 - 350 cP | 250 - 350 cP | |
|
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||