| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
350000
-
450000
cP @Temperature 25.0 °C |
350000
-
450000
cP @Temperature 77.0 °F |
|
|
Nanocyl EPOCYL™ NC E128-02 Master Batch Liquid Bisphenol-A Resin for non-Solvent Based Formulation Purposes
EPOCYL™ NC E128-02 is a Mater Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enh..
|
|||
| Viscosity |
350000
-
450000
cP @Temperature 25.0 °C |
350000
-
450000
cP @Temperature 77.0 °F |
|
|
Nanocyl EPOCYL™ NC R128-02 Master Batch Liquid Bisphenol-A Resin for Hot-Melt Formulation Purposes: Dilution Factor 6
EPOCYL™ NC R128-02 is a Master Batch based on liquid Bisphenol-A (Bis-A) epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of..
|
|||
| Viscosity | 350000 - 550000 cP | 350000 - 550000 cP | Paste |
|
ND Industries 460 Instant High Pressure Pipe Sealant
High temperature, high strength general purpose stainless steel and other inert metals. For metal fittings
|
|||
| Viscosity |
350000
cP @Temperature 200 °C |
350000
cP @Temperature 392 °F |
melt; 1000 sec-1; ASTM D 3825 |
|
SABIC Innovative Plastics Cycolac® FR30U ABS
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Viscosity |
350000
cP @Temperature 400 °C |
350000
cP @Temperature 752 °F |
Melt; ISO 11443 |
|
Victrex® HT™ P45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co..
|
|||
| Viscosity |
350000
cP @Temperature 400 °C |
350000
cP @Temperature 752 °F |
melt; ISO 11443 |
|
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE
Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo..
|
|||
| Viscosity |
350000
cP @Temperature 400 °C |
350000
cP @Temperature 752 °F |
ISO 11443 |
|
Victrex® PEEK 450PF Fine Powder Grade
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia..
|
|||
| Viscosity |
350000
-
600000
cP @Temperature 220 - 220 °C |
350000
-
600000
cP @Temperature 428 - 428 °F |
Average value: 475000 cP Grade Count:2 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
|
|||
| Viscosity |
350000
-
350000
cP @Temperature 200 - 200 °C |
350000
-
350000
cP @Temperature 392 - 392 °F |
Average value: 223000 cP Grade Count:1 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
|
|||
| Viscosity |
350000
cP @Shear Rate 1000 1/s, Temperature 400 °C |
350000
cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
|
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber
KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS..
|
|||
| Viscosity | >= 350000 cP | >= 350000 cP | Part A |
|
Master Bond MasterSil 153Med Silicone Paste for Medical Applications
Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it..
|
|||
| Viscosity | 350000 cP | 350000 cP | |
|
Loctite® PST® 592 Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
|
|||
| Viscosity |
350000
cP @Shear Rate 0.100 1/s, Temperature 280 °C |
350000
cP @Shear Rate 0.100 1/s, Temperature 536 °F |
|
|
DSM Akulon® F127 PA6
Low/Medium Viscosity, Film Extrusion
|
|||
| Viscosity |
350000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F130-C PA6
Film Extrusion, Medium Viscosity, Lubricated
|
|||
| Viscosity |
350000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F130-C2 PA6
Medium Viscosity, Film Extrusion, Lubricated
|
|||
| Viscosity |
350000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F130-C3 PA6
Monofilament Grade, Extrusion Grade, Medium Viscosity, Lubricated
|
|||
| Viscosity |
350000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock
|
|||
| Viscosity |
350000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F132-E1 PA6
Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
|
|||
| Viscosity |
350000
cP @Shear Rate 1000 1/s, Temperature 260 °C |
350000
cP @Shear Rate 1000 1/s, Temperature 500 °F |
|
|
DSM Akulon® F132-E2 PA6
High Viscosity, Nucleated, Lubricated, Film Extrusion
|
|||
| Viscosity |
350000
cP @Temperature 160 °C |
350000
cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
|
EMS-Griltech Griltex® 9E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
|
|||
| Viscosity |
350000
-
550000
cP @Temperature 23.0 °C |
350000
-
550000
cP @Temperature 73.4 °F |
0.5 rpm |
|
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive
Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400..
|
|||
| Viscosity |
350000
cP @Shear Rate 1.00 1/s, Temperature 23.0 °C |
350000
cP @Shear Rate 1.00 1/s, Temperature 73.4 °F |
|
|
Dow BETAMATE™ XW 1185 Epoxy
BETAMATE™ XW 1185 is a one component heat curing Epoxy paste adhesive. The material is readily pumped at ambient temperatures. It shows excellent adhesion to automotive steel and aluminum, is resi..
|
|||
| Viscosity |
350000
cP @Shear Rate 300 1/s, Temperature 190 °C |
350000
cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
|
Advanced Polymer Alloys Alcryn® 2060 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
|
|||
| Viscosity |
350000
cP @Temperature 25.0 °C |
350000
cP @Temperature 77.0 °F |
After mixing |
|
Tra-Con Tra-Bond 224-8 Room Temperature Cure Epoxy Adhesive
TRA-BOND 224-8 room temperature cure epoxy adhesive is a thermally conductive version of 224-1. This adhesive develops structural strength rapidly. When cured at room temperature, this adhesive prov..
|
|||
| Viscosity |
350000
-
850000
cP @Temperature 400 - 400 °C |
350000
-
850000
cP @Temperature 752 - 752 °F |
Average value: 445000 cP Grade Count:3 |
|
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
|
|||
| Viscosity |
350000
-
850000
cP @Shear Rate 1000 - 1000 1/s |
350000
-
850000
cP @Shear Rate 1000 - 1000 1/s |
Average value: 445000 cP Grade Count:3 |
|
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
|
|||
| Viscosity | 350000 cP | 350000 cP | Mixed; TM R050-12 |
|
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive
EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go..
|
|||
| Viscosity | 350000 - 700000 cP | 350000 - 700000 cP | |
|
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F
Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4..
|
|||