| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 40 cP | 40 cP | |
|
Ritelok EC40 General Purpose Ethyl CA Adhesive
Cyanoacrylate. General purpose, cures instantly on rubbers, plastics, & many other materials. High Strength, Medium viscosity, Penetrating action
|
|||
| Viscosity | 40 cP | 40 cP | Fed Std Method 4287 |
|
Humiseal 1B12 Acrylic Conformal Coating
Humiseal 1B12 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityPasses thermal shock test (MIL-I-46058C)Flammabili..
|
|||
| Viscosity | 40 - 70 cP | 40 - 70 cP | |
|
Huntsman HY 2964 Cycloaliphatic Amine
Approx. H+ equivalent weight 93. Mix Ratio with GY 6010 is 50.Comments/Applications: Very low viscosity modified aliphatic amine for solvent free high performance applications. Light color, blush..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
KKPC KOSYN KSL 315 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: KOSYN KSL 300 series is a Styrene-Butadiene Latex.Applications: Oil-resistant Foam Rubber, For Impregnation of Tire and Belt Cord, Foam Backing of Textile Goo..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
KKPC KOSYN KSL 601 Styrene-Butadiene Latex
Styrene-Butadiene LatexCharacteristics: High adhesive strength, excellent printing aptitude, excellent adhesive degree, heat resistance, good dispersion, foam stability, aging resistance, good a..
|
|||
| Viscosity |
40
-
120
cP <br>@Temperature 25.0 °C
|
40
-
120
cP <br>@Temperature 77.0 °F
|
|
|
Lord Adhesives Flocklok® 870 Flock Adhesive
LORD Flocklok® 870 adhesive is a single-coat adhesive used to adhere polyester or nylon flock if beers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good r..
|
|||
| Viscosity | 40 cP | 40 cP | B-type viscometer (60rpm) |
|
Mitsui UNISTOLEâ„¢ R-300 Polyolefinic Primer/ Adhesive
UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi..
|
|||
| Viscosity |
40
-
275
cP <br>@Temperature 25.0 °C
|
40
-
275
cP <br>@Temperature 77.0 °F
|
|
|
Lord Adhesives Flocklok® 855 Flock Adhesive
LORD Flocklok® 855 adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of elastomers including EPDM, NR, CR and SBR. Flocked substrates provide good res..
|
|||
| Viscosity |
40
cP <br>@Temperature 30.0 °C
|
40
cP <br>@Temperature 86.0 °F
|
10% wt, Toluene Solution |
|
Kuraray SEPTON® S8004 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
|
|||
| Viscosity | >= 40 cP | >= 40 cP | |
|
Solvay Chemicals NOCOLOK® Precoating (water soluble)
NOCOLOK® Precoating can be used in mixture with NOCOLOK® Flux or NOCOLOK® Zn Flux and water to improve adhesion of the flux coating. Uses: Automotive Sector, Commercial & Residential Air C..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
Solvay ANTAROX® BL 225 Surfactant
Description: Biodegradable linear alcohol EO/PO. Low foaming non-ionic with excellent hard surface detergency combined to wetting properties. Soluble in water and most organic solvents except paraff..
|
|||
| Viscosity | 40 - 90 cP | 40 - 90 cP | NOV QC 020 |
|
Lubrizol ESTANE® 5799 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
Elmer's Products Aron Alpha® 241F Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
Elmer's Products Aron Alpha® 241 Cyanoacrylate Adhesive (Industrial Krazy Glue™)
General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
Elmer's Products Aron Alpha® 241E Cyanoacrylate Adhesive (Industrial Krazy Glue™)
For clean, fast applications. Best for high speed automated assembly.Low gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. Excellent on porous subs..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
BASF Lupranate® MM103 Isocyanate Modified MDI
Description: Lupranate® MM103 is a liquid carbodiimide modified 4,4’-diphenylmethane diisocyanate. Lupranate MM103 serves as the isocyanate component in the production of microcellular urethane el..
|
|||
| Viscosity | 40 cP | 40 cP | B Component; ASTM D1824 |
|
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive
Space Grade, Low modulus urethane ESD coating/adhesiveAPTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an elect..
|
|||
| Viscosity | 40 cP | 40 cP | ASTM D1824 |
|
Aptek 7503LM-PMF UV Urethane Conformal Coating
UV-cured, low modulus, shadow cures under components. Excellent adhesion without primer. Repairable. Qualified to MIL-I-46058C, types UR and AR. Castable version – UVIKOTE 7504 LM-PMF.Information p..
|
|||
| Viscosity | 40 - 100 cP | 40 - 100 cP | |
|
Beijing Ranger Chem 6690-4 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
|
|||
| Viscosity | 40 - 50 cP | 40 - 50 cP | |
|
Aremco Lamp-Coat™ LC4010-BT High Temperature Coating, Silicone
Aluminum-filled coating for application over black top coated headlamps to 1020 °F (550 °C).
|
|||
| Viscosity | 40 cP | 40 cP | |
|
BASF Lupranate® 219 Isocyanate Modified MDI
Description: Lupranate® 219 Isocyanate is a liquid carbodiimide modified 4,4’-diphenylmethane diisocyanate. Lupranate 219 Isocyanate is a light-colored alternative to Lupranate MM103 Isocyanate. ..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
BASF Lupranate® 81 Isocyanate
Description: Lupranate® 81 Isocyanate is a carbodiimide modified pure MDI with a higher 2,4’-isomer content and a functionality of approximately 2.1. Lupranate 81 Isocyanate exhibits good low temp..
|
|||
| Viscosity |
40
cP <br>@Temperature 75.0 °C
|
40
cP <br>@Temperature 167 °F
|
|
|
ACC EP A 32 EPI Engineered Polymers MDI
EP A 32, “Powered by Reactamine® Technology”, is a mixture of 4,4 and 2,4 MDI with a low viscosity. EP A 32 has stability at low temperatures, and is useful for making elastomers and prepolymers...
|
|||
| Viscosity | 40 cP | 40 cP | |
|
3M Scotch-Weld™ HT40 High Temperature Instant Adhesive
3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT40 is a low..
|
|||
| Viscosity | 40 - 80 cP | 40 - 80 cP | |
|
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass
Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C)
|
|||
| Viscosity | 40 - 80 cP | 40 - 80 cP | |
|
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating
3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri..
|
|||
| Viscosity | 40 cP | 40 cP | |
|
BASF Lupranate® 5143 Isocyanate
Description: Lupranate® 5143 isocyanate is a liquid, carbodiimide-modified 4,4’-diphenylmethane diisocyanate. With manufacturing advances, Lupranate 5143 isocyanate achieves better low temperature..
|
|||
| Viscosity | 40 - 120 cP | 40 - 120 cP | RP-0596 |
|
Solvay RHODAPON® TL-40/A Surfactant
Description: Rhodapon® TL-40/A is formaldehyde preserved clear light liquid with excellent foaming characteristics. It is a milder Lauryl sulfate grade and it has enhanced compatibility with fragra..
|
|||