| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
150
-
400
cP @Temperature 30.0 °C |
150
-
400
cP @Temperature 86.0 °F |
|
|
Prodways PLASTCure ABS 3650 3D Printing Polymer
Good chemical resistance. High transparency.Ideal for segments such like medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accur..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | 15% solution in MEK |
|
Lubrizol Advanced Materials Pearlstick® 46-10/03 Polyester based TPU
(discontinued **)
TPUs for Solvent-based adhesivesApplications: Others, FurnitureInformation provided by Merquinsa
|
|||
| Viscosity |
100
-
400
cP @Temperature 45.0 °C |
100
-
400
cP @Temperature 113 °F |
|
|
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity |
100
-
400
cP @Temperature 45.0 °C |
100
-
400
cP @Temperature 113 °F |
|
|
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity | 20 - 400 cP | 20 - 400 cP | |
|
Kazanorgsintez NMPE-2 Low-Molecular Polyethylene
Notes: Low-molecular polyethylene of high pressure polyethylene production. Application: Designed for use in the rubber industry, building industry, and other fields. Can also be used as compon..
|
|||
| Viscosity | 250 - 400 cP | 250 - 400 cP | |
|
Huntsman HY 355 Cycloaliphatic Amine
Approx. H+ equivalent weight 48.5. Mix Ratio with GY 6010 is 26.Comments/Applications: Modified cycloaliphatic polyamine adduct for resistance to solvents and high temperature, especially when use..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | 25% Toluene Solution at 25°C; BAM 922 |
|
Kraton® D1164 P (SIS) Linear Triblock Copolymer
Description: Kraton D1164 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 29%. It is supplied from North America in the physical form identified: ..
|
|||
| Viscosity | 280 - 400 cP | 280 - 400 cP | 25% Toluene Solution at 25°C; BAM 922 |
|
Kraton® D1124 P (SIS) Branched Copolymer
Description: Kraton D1124 P is a clear, branched copolymer based on styrene and isoprene with a polystyrene content of 30%. It is supplied from North America in the physical form identified: Kraton ..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | ASTM D803 |
|
SK Chemicals SKYTHANE® US230 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Viscosity |
300
-
400
cP @Temperature 23.0 °C |
300
-
400
cP @Temperature 73.4 °F |
|
|
Master Bond EP112 Low Viscosity Structural Epoxy Adhesive System
Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical and..
|
|||
| Viscosity | 300 - 400 cP | 300 - 400 cP | Part B |
|
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy
Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N..
|
|||
| Viscosity |
300
-
400
cP @Temperature 23.0 °C |
300
-
400
cP @Temperature 73.4 °F |
|
|
Master Bond EP37-3 Optically Clear, Impact Resistant Two Component Epoxy
Master Bond Polymer System EP37-3 is a low viscosity, resilient, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. As an adhes..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | Part B |
|
Master Bond EP38CL Adhesive Features Toughness and Durability
Description: Master Bond EP38CL is a lower viscosity, optically clear two component epoxy system for high performance bonding, coating, sealing and small encapsulations, featuring toughness and dura..
|
|||
| Viscosity | 250 - 400 cP | 250 - 400 cP | Part B |
|
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating
Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to..
|
|||
| Viscosity |
300
-
400
cP @Temperature 125 °C |
300
-
400
cP @Temperature 257 °F |
TXAL-A-XX-G-V-005 |
|
Westlake Epolene® E-14P Oxidized Low Molecular Weight Polyethylene Polymer
Description: The Epolene E-14P is a low molecular-weight, low-density, oxidized polyethylene powder. It is useful as a lubricant in processing rigid and flexible polyvinyl chloride (PVC) and as a pr..
|
|||
| Viscosity |
100
-
400
cP @Temperature 45.0 °C |
100
-
400
cP @Temperature 113 °F |
|
|
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity |
100
-
400
cP @Temperature 45.0 °C |
100
-
400
cP @Temperature 113 °F |
|
|
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity | 300 - 400 cP | 300 - 400 cP | Part B |
|
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
|
|||
| Viscosity |
300
-
400
cP @Temperature 23.0 °C |
300
-
400
cP @Temperature 73.4 °F |
|
|
Master Bond UV10 One Component UV Curable Adhesive System
Master Bond UV10 is a multi-purpose, one part UV type system for bonding, sealing and coating that features good optical clarity and physical properties as well as an exceptionally low viscosity. UV..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | |
|
Epoxyset Epoxibond EB-107LP-1 Unfilled Epoxy Adhesive
A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc.
|
|||
| Viscosity | 100 - 400 cP | 100 - 400 cP | |
|
Abatron BestBond® Waterborne Polyurethane Adhesive for Wood
BestBond® is a versatile adhesive designed for both interior and exterior wood projects. BestBond® is water-resistant, easy to clean up, non-toxic, and flexible. Primary suggested uses include fur..
|
|||
| Viscosity | 300 - 400 cP | 300 - 400 cP | |
|
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | |
|
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | |
|
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass
Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C)
|
|||
| Viscosity | 300 - 400 cP | 300 - 400 cP | |
|
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone
Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC)
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | |
|
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..
|
|||
| Viscosity | 300 - 400 cP | 300 - 400 cP | |
|
BASF Lupranate® 277 Isocyanate
Description: Lupranate® 277 Isocyanate is a medium viscosity polymeric MDI isocyanateInformation provided by BASF
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | |
|
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95%
This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo..
|
|||
| Viscosity | 200 - 400 cP | 200 - 400 cP | 15% solution in MEK |
|
Lubrizol Advanced Materials Pearlstick® 45-40/03 Polycaprolactone based TPU
(discontinued **)
TPUs for Solvent-based adhesivesApplications: Automotive, OthersInformation provided by Merquinsa
|
|||