| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
400
-
800
cP @Temperature 25.0 °C |
400
-
800
cP @Temperature 77.0 °F |
cPs |
|
Oceanchem Group Resorcinol bis (Diphenyl Phosphate) (RDP)
Molecular Formula: C30H24O8P2Cas No.: 57583-54-7RDP is a halogen-free phosphorus-based flame retardant.Use:RDP flame retardant provides a halogen-free solution for flame retarding PC/ABS, PPO/HIPS a..
|
|||
| Viscosity | 400 - 800 cP | 400 - 800 cP | |
|
ND Industries 560 Shaft & Bearing Retainer Retaining Compound
High Temperature retainer for bushings and sleeves. Retains rotors to shaftsMeets military spec Mil-R-46082B Type II
|
|||
| Viscosity |
400
cP @Temperature 25.0 °C |
400
cP @Temperature 77.0 °F |
Uncured |
|
Permabond 265 Cyanoacrylate
PERMABOND 265 is a medium viscosity cyanoacrylate ideal for intermediate gap fill application. PERMABOND 265 provides faster set times and improved gap-filling capability compared to conventional cy..
|
|||
| Viscosity | 400 - 530 cP | 400 - 530 cP | 20% Toluene Solution at 25°C; KM 06 |
|
Kraton® G1652 E (SEBS) Linear Triblock Copolymer
Description: Kraton G1652 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical ..
|
|||
| Viscosity | 400 - 525 cP | 400 - 525 cP | 20% Toluene Solution at 25°C; BAM 922 |
|
Kraton® G1652 M (SEBS) Linear Triblock Copolymer
Description: Kraton G1652 M is a translucent, linear triblock copolymer based on styrene and ethylene/butylene (SEBS) with a Styrene / Rubber ratio of 30/70. It is supplied from North America in the..
|
|||
| Viscosity | 400 cP | 400 cP | Part B |
|
Multibase 7-9600 Dow-Corning Soft Filling Elastomer Parts A and B
Information provided by Multibase
|
|||
| Viscosity |
400
-
680
cP @Temperature 25.0 °C |
400
-
680
cP @Temperature 77.0 °F |
|
|
Struktol STRUKSILON 8017 Silicone Stabilizer for PU-Rigid Foam
STRUKSILON 8017 was developed as specific silicone stabilizer for continuous production of PIR based rigid foam materials.Applications: STRUKSILON 8017 is applicable in combination with HCFC’s ..
|
|||
| Viscosity |
400
-
500
cP @Temperature 23.0 °C |
400
-
500
cP @Temperature 73.4 °F |
|
|
Master Bond EP30 Optically Clear, Low Viscosity Two Component Epoxy
Master Bond Polymer System EP30 is a low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at room temperature or more..
|
|||
| Viscosity | 400 - 500 cP | 400 - 500 cP | mixed |
|
Master Bond EP37-3FLSP Optically Clear Epoxy Has Low Exotherm
Description: Master Bond EP37-3FLSP is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. It fe..
|
|||
| Viscosity |
400
cP @Temperature 25.0 °C |
400
cP @Temperature 77.0 °F |
After mixing |
|
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound
TRA-CAST 3143 has a low viscosity and long pot life. It is certified to the requirements of UL 94 V-O, and is recommended for rigid potting, laminating, transformer encapsulating, filament winding a..
|
|||
| Viscosity | 400 cP | 400 cP | dynamic |
|
Dow Corning 7-9600 A&B SOFT FILLING ELASTOMER KIT
Two-part, platinum-catalyzed, unfilled silicone elastomer commonly used to fill external form prostheses and pressure cushions.Information provided by Dow Corning
|
|||
| Viscosity | 400 cP | 400 cP | dynamic |
|
Dow Corning 7-9800 SOFT SKIN ADHESIVE KIT (A&B)
Two-part, platinum-catalyzed, unfilled silicone elastomeric adhesive. This a clear and soft skin adhesive for wound care dressings, transdermal drug delivery, or pharmaceutical topical applications...
|
|||
| Viscosity | 400 cP | 400 cP | dynamic |
|
Dow Corning SE 1885 KIT
Two-part, clear, 1:1, addition cure, low temperature cure, low temperature capable, low viscosity.Information provided by Dow Corning
|
|||
| Viscosity | 400 cP | 400 cP | Dynamic |
|
Dow Corning SYL-OFF® PMCPSL 9104 Coating
Syl-Off® SL 9104 Coating is a solvent-free silicone release coating for polyester substrates, providing excellent long-term anchorage to a wide range of both primed and unprimed polyester films.Inf..
|
|||
| Viscosity | 400 - 550 cP | 400 - 550 cP | Dynamic |
|
Dow Corning 20 Demethiconol Blend
A unique blend of silicone gum (6%) in dimethicone for use in a wide range of skin care and topical pharmaceutical applications.Information provided by Dow Corning
|
|||
| Viscosity |
400
-
600
cP @Temperature 25.0 °C |
400
-
600
cP @Temperature 77.0 °F |
|
|
BorsodChem ONGRONAT PE-191 MDI Isocyanate
Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyester-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for p..
|
|||
| Viscosity | 400 - 800 cP | 400 - 800 cP | Mixed Viscosity |
|
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Viscosity | 400 - 600 cP | 400 - 600 cP | blended |
|
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
|
|||
| Viscosity | 400 - 600 cP | 400 - 600 cP | |
|
3M Scotch-Weld™ CA40H Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity version of CA40 and better void filling capabilities.Information provided by 3M
|
|||
| Viscosity | 400 - 700 cP | 400 - 700 cP | |
|
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, white coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadi..
|
|||
| Viscosity | 400 - 600 cP | 400 - 600 cP | |
|
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
| Viscosity | 400 - 800 cP | 400 - 800 cP | |
|
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a..
|
|||
| Viscosity | 400 - 900 cP | 400 - 900 cP | |
|
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone
Low viscosity, white coating for motor windings to 1100°F (593°C)
|
|||
| Viscosity |
400
-
600
cP @Temperature 23.9 °C |
400
-
600
cP @Temperature 75.0 °F |
|
|
TSE Industries EzNATE® 100 Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
|
|||
| Viscosity |
400
cP @Temperature 25.0 °C |
400
cP @Temperature 77.0 °F |
Uncured |
|
Permabond A118 Anaerobic Retainer
Permabond® A118 is an anaerobic adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It exhibits high strength, ex..
|
|||