| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
140
-
40000
cP @Temperature 121 - 190 °C |
140
-
40000
cP @Temperature 250 - 374 °F |
Average value: 495000 cP Grade Count:42 |
|
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
|
|||
| Viscosity | 6000 - 40000 cP | 6000 - 40000 cP | |
|
Huntsman Araldite GZ 540 X-90 Bisphenol A Epoxy Solution
Weight per Epoxide (EEW, g/eq) 233 to 278. Max color is 3.Comments/Applications: GY 6040 - 90% solids in xylene. General purpose bis A epoxy solution for use in 2-package maintenance and architect..
|
|||
| Viscosity | 6000 - 40000 cP | 6000 - 40000 cP | |
|
Huntsman Araldite GZ 6097 PM-55 Bisphenol A Epoxy Solution
Weight per Epoxide (EEW, g/eq) 2000 to 2500. Max color is 3.Comments/Applications: GZ 6097 - 55% solids in PM (propylene glycol monomethyl ether). Much higher flexibility and toughness than GT 707..
|
|||
| Viscosity |
25000
-
40000
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
25000
-
40000
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2090428D4 Gold Ink
Gold Ink is a fritted system that has been designed as a screen printing ink for uses on Alumina. It is also suitable for firing onto other high temperature substrates. This product should be used ..
|
|||
| Viscosity |
25000
-
40000
cP @Temperature 40.0 °C |
25000
-
40000
cP @Temperature 104 °F |
|
|
Taiwan PU Corporation PPG CPU-2172 Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
|
|||
| Viscosity | 30000 - 40000 cP | 30000 - 40000 cP | |
|
Master Bond MasterSil 709 One Part Silicone Meets MIL Spec
Description: MasterSil 709 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This unique product meets the MIL..
|
|||
| Viscosity | 25000 - 40000 cP | 25000 - 40000 cP | Part A |
|
Master Bond EP30QF Quartz Filled, Two Component Epoxy System
Master Bond Polymer System EP30QF is a quartz filled, two component epoxy for high performance bonding, sealing, coating and casting that is formulated to cure at room temperature or more rapidly at..
|
|||
| Viscosity |
30000
-
40000
cP @Temperature 23.0 °C |
30000
-
40000
cP @Temperature 73.4 °F |
|
|
Master Bond Supreme 11 High Peel and Shear Strength Epoxy Adhesive
Master Bond Polymer System Supreme 11 features a unique balance of performance properties including both high shear and high peel strengths. This two component adhesive system is formulated to cure ..
|
|||
| Viscosity |
30000
-
40000
cP @Temperature 23.0 °C |
30000
-
40000
cP @Temperature 73.4 °F |
|
|
Master Bond UV10TK Dimensionally Stable One Component UV Curable Adhesive
Master Bond UV10TK is a moderate viscosity, one part UV system for bonding, sealing and coating featuring very good optical clarity and excellent physical properties as well as superior temperature ..
|
|||
| Viscosity |
20000
-
40000
cP @Temperature 21.0 °C |
20000
-
40000
cP @Temperature 69.8 °F |
|
|
Abatron AboCast/AboCure 8109-12
1-part, contains latent hardener activated by higher temperature. 4-6 month shelf life at 20-25°C (68-77°F). Other versions available with longer shelf lives and cure cycles.Processing: Potlife:..
|
|||
| Viscosity | 20000 - 40000 cP | 20000 - 40000 cP | |
|
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Viscosity | 30000 - 40000 cP | 30000 - 40000 cP | |
|
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||
| Viscosity | 20000 - 40000 cP | 20000 - 40000 cP | |
|
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
|
|||