Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 44 - 50 cP
<br>@Temperature 20.0 °C
44 - 50 cP
<br>@Temperature 68.0 °F
4% solids aqueous solution, Hoeppler falling ball method
DuPont Elvanol® 50-42 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade
Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late..