| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity |
30
-
50
cP <br>@Temperature 25.0 °C
|
30
-
50
cP <br>@Temperature 77.0 °F
|
Uncured |
|
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
|
|||
| Viscosity |
30
-
50
cP <br>@Temperature 25.0 °C
|
30
-
50
cP <br>@Temperature 77.0 °F
|
Uncured |
|
Permabond 791 Cyanoacrylate, Surface insensitive
PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..
|
|||
| Viscosity | 15 - 50 cP | 15 - 50 cP | As Supplied |
|
Heraeus Cleviosâ„¢ PH 1000 Conductive Sulfonate Polymer for Antistatic Coatings
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PH 1000 is an antistatic material based on PED..
|
|||
| Viscosity |
44
-
50
cP <br>@Temperature 20.0 °C
|
44
-
50
cP <br>@Temperature 68.0 °F
|
4% solids aqueous solution, Hoeppler falling ball method |
|
DuPont Elvanol® 50-42 Polyvinyl Alcohol Partially Hydrolyzed General Purpose Grade
Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late..
|
|||
| Viscosity | 30 - 50 cP | 30 - 50 cP | |
|
Chesterton 415 Concrete Sealer
Chesterton® 415 Concrete Sealer is a high gloss, fast penetrating coating which forms a polymeric seal over surfaces to which it is applied. When used on porous surfaces such as concrete floors, wa..
|
|||
| Viscosity | 40 - 50 cP | 40 - 50 cP | |
|
Aremco Lamp-Coat™ LC4010-BT High Temperature Coating, Silicone
Aluminum-filled coating for application over black top coated headlamps to 1020 °F (550 °C).
|
|||