| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | |
|
Huntsman Araldite EPN 1138 Epoxy Phenol Novolac
Weight per Epoxide (EEW, g/eq) 176 to 181. Max color is 2.Comments/Applications: Epoxy phenol novolac for higher heat and chemical resistance than PY 307-1 and EPN 1139 or EPN 1179. Used in coatin..
|
|||
| Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | |
|
Huntsman Araldite EPN 1180 Epoxy Phenol Novolac
Weight per Epoxide (EEW, g/eq) 175 to 182. Max color is 2.Comments/Applications: Epoxy functionality of 3.6. Much higher viscosity than EPN 1139 or EPN 1179. For higher heat and chemical resistan..
|
|||
| Viscosity | 30000 - 50000 cP | 30000 - 50000 cP | |
|
Huntsman Araldite PY 307-1 Epoxy Phenol Novolac
Weight per Epoxide (EEW, g/eq) 170 to 179. Max color is 4.Comments/Applications: Epoxy functionality of 2.4. EPN 1139 or EPN 1179 type with much lower viscosity. FDA listed. For high performance..
|
|||
| Viscosity |
35000
-
50000
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
35000
-
50000
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C1991025D2 Gold Ink
Gold Ink C1991025D2 is a fritted system that has been designed as a screen printing ink for uses on alumina. It is also suitable for firing onto other high temperature substrates. This product shou..
|
|||
| Viscosity |
40000
-
50000
cP @Temperature 23.0 °C |
40000
-
50000
cP @Temperature 73.4 °F |
|
|
Master Bond EP21TDC Toughened, Shock Resistant Two Component Epoxy System
Master Bond Polymer Adhesive EP21TDC is a two component epoxy adhesive for general purpose bonding formulated to cure at room temperature or more rapidly at elevated temperatures, with a one-to-one ..
|
|||
| Viscosity |
40000
-
50000
cP @Temperature 23.0 °C |
40000
-
50000
cP @Temperature 73.4 °F |
|
|
Master Bond EP30D-7 Flexibilized, Abrasion Resistant Epoxy System
Master Bond Polymer System EP30D-7 is a versatile two component flexibilized, urethane-modified epoxy featuring superior strength, toughness and abrasion resistance for high performance bonding, sea..
|
|||
| Viscosity |
40000
-
50000
cP @Temperature 23.0 °C |
40000
-
50000
cP @Temperature 73.4 °F |
|
|
Master Bond EP45HT High Temperature Resistant, Electrically Insulating Epoxy
Master Bond Polymer System EP45 is a two component epoxy system for high performance structural bonding and casting suitable for applications where long term exposure to temperatures from -80° to +..
|
|||
| Viscosity |
5000
-
50000
cP @Temperature 120 °C |
5000
-
50000
cP @Temperature 248 °F |
|
|
Abatron AboCast/AboCure 8109-2
High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°..
|
|||
| Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
|
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
|
|||
| Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
|
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
|
|||
| Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
|
3M Scotch-Weld™ DP420 LH Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
|
|||
| Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
|
3M Scotch-Weld™ DP420 NS Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
|
|||
| Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | Base |
|
3M Scotch-Weld™ DP405 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel..
|
|||
| Viscosity | 17000 - 50000 cP | 17000 - 50000 cP | Thixotropic |
|
Loctite® 572 Low Strength Thread Sealant
Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p..
|
|||
| Viscosity | 20000 - 50000 cP | 20000 - 50000 cP | |
|
Beijing Ranger Chem SM-602RX75 Solvent Based Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
|
|||