| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 500000 cP | 500000 cP | Part A, RVT, #7, 2.5 rpm; TM R050-12 |
|
Resinlab® EP1121-4 Adhesive / Casting Resin
Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives ..
|
|||
| Viscosity |
500000
cP @Shear Rate 250 1/s, Temperature 230 °C |
500000
cP @Shear Rate 250 1/s, Temperature 446 °F |
|
|
Noltex Soarnol® D2908 Ethylene Vinyl Alcohol Copolymer
Ethylene content 29 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a..
|
|||
| Viscosity | 500000 cP | 500000 cP | RVT, #7, 2.5 rpm; TM R050-12 |
|
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
|
|||
| Viscosity | 500000 cP | 500000 cP | RVT, #7, 2.5 rpm; TM R050-12 |
|
Resinlab® EP1330 Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
|
|||
| Viscosity |
500000
cP @Temperature 400 °C |
500000
cP @Temperature 752 °F |
Melt; ISO 11443 |
|
Victrex® PEEK 600G Polyetheretherketone
(discontinued **)
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta..
|
|||
| Viscosity |
500000
cP @Temperature 400 °C |
500000
cP @Temperature 752 °F |
melt; ISO 11443 |
|
Victrex® PEEK 650P PolyEtherEtherKetone
High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, color natural.Info..
|
|||
| Viscosity |
500000
cP @Shear Rate 50.0 1/s, Temperature 190 °C |
500000
cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
|
DuPont Bynel® 3120 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **)
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
|
|||
| Viscosity |
500000
cP @Shear Rate 50.0 1/s, Temperature 190 °C |
500000
cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
|
DuPont Bynel® E326 Acid-/Acrylate-Modified EVA Adhesive Resin
(discontinued **)
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
|
|||
| Viscosity | 500000 - 800000 cP | 500000 - 800000 cP | |
|
Lord Adhesives 310 High Strength SMC, FRP and General Purpose Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
|
|||
| Viscosity |
500000
cP @Temperature 130 °C |
500000
cP @Temperature 266 °F |
Melt; ISO 1133 |
|
Lubrizol Advanced Materials PEARLBOND® 503 Linear Thermoplastic Polyurethane
Pearlbondâ„¢ 503 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli..
|
|||
| Viscosity | 500000 cP | 500000 cP | Melt Viscosity; ASTM D3835 |
|
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi..
|
|||
| Viscosity | 500000 cP | 500000 cP | B |
|
Shin-Etsu Silicones LIMSâ„¢ KE1950-35A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
|
|||
| Viscosity | 500000 cP | 500000 cP | Mixed |
|
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive
TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar..
|
|||
| Viscosity | 500000 cP | 500000 cP | dynamic |
|
Dow Corning 7-3105 PERTOLATUM HIP EMULSION
A concentrated emulsion of petrolatum (USP) that is designed to facilitate the rapid development of skin care formulations which contain this emollient. Typical applications include: suncare, body l..
|
|||
| Viscosity | <= 500000 cP | <= 500000 cP | Dynamic |
|
Dow Corning SE 4490 CV
One-part, white, non-flowing, highly filled compound, excellent thermal conductivity.Information provided by Dow Corning
|
|||
| Viscosity |
500000
cP @Temperature 160 °C |
500000
cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
|
EMS-Griltech Griltex® 11A Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
|
|||
| Viscosity |
500000
cP @Temperature 160 °C |
500000
cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
|
EMS-Griltech Griltex® D 1556A Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
|
|||
| Viscosity |
500000
cP @Temperature 160 °C |
500000
cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
|
EMS-Griltech Griltex® D 1712A Copolyamide Hotmelt Adhesive (Apparel Interlinings)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
|
|||
| Viscosity |
500000
cP @Shear Rate 1.00 1/s, Temperature 40.0 °C |
500000
cP @Shear Rate 1.00 1/s, Temperature 104 °F |
cone/plate |
|
Dow BETAMATE™ 1496 V Epoxy
BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excelle..
|
|||
| Viscosity | 500000 cP | 500000 cP | Mixed |
|
Armstrong A-3/A Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
|
|||
| Viscosity | 500000 cP | 500000 cP | Mixed |
|
Armstrong A-4/E Epoxy Adhesive
Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhe..
|
|||
| Viscosity |
500000
cP @Shear Rate 300 1/s, Temperature 190 °C |
500000
cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
|
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
|
|||
| Viscosity |
500000
-
1.60e+6
cP @Shear Rate 100 1/s, Temperature 232 °C |
500000
-
1.60e+6
cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
|
Arkema Group KYNAR FLEX® 2500-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Highest flexibility. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical st..
|
|||
| Viscosity |
500000
-
1.20e+6
cP @Shear Rate 100 1/s, Temperature 232 °C |
500000
-
1.20e+6
cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
|
Arkema Group KYNAR® 721 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
|
|||
| Viscosity |
500000
-
800000
cP @Shear Rate 100 1/s, Temperature 232 °C |
500000
-
800000
cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
|
Arkema Group KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
|
|||
| Viscosity |
500000
cP @Temperature 180 °C |
500000
cP @Temperature 356 °F |
Melt; Flowtester (100 kgf/cm², dimension of die 1 &#934; mm x 10 mm) |
|
Zeon Chemicals Quintac® 3433N SIS Block Polymer
Styrene Isoprene (SIS) Block Polymer. Information provided by Zeon Chemicals L.P.
|
|||
| Viscosity |
500000
-
800000
cP @Shear Rate 100 1/s, Temperature 232 °C |
500000
-
800000
cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
|
Arkema Group KYNAR FLEX® 2850 PC Polyvinylidene Fluoride Spray Coating Powder
Electrostatic sprayInformation provided by Arkema Inc.
|
|||
| Viscosity | 500000 cP | 500000 cP | Part A, RVT, #7, 2.5 rpm; TM R050-12 |
|
Resinlab® EP1305 Black Highly Toughened Urethane Modified Epoxy
Resinlab™ EP1305 Black is a highly toughened urethane modified epoxy designed for bonding PVC, metals, ceramics and other difficult to bond substrates. The system has a thixotropic non-sag viscosi..
|
|||
| Viscosity |
500000
cP @Shear Rate 50.0 1/s, Temperature 190 °C |
500000
cP @Shear Rate 50.0 1/s, Temperature 374 °F |
|
|
DuPont Nucrel® 1207 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinued
12 wt% Methacrylic Acid.Nucrel® 1207 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des..
|
|||