Polymer Property : Viscosity = 550000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 150000 - 550000 cP
150000 - 550000 cP
Paste
ND Industries 420 Instant High Pressure Pipe Sealant
Industrial grade, controlled locking strength for metal fittings
Viscosity 350000 - 550000 cP
350000 - 550000 cP
Paste
ND Industries 460 Instant High Pressure Pipe Sealant
High temperature, high strength general purpose stainless steel and other inert metals. For metal fittings
Viscosity 350000 - 550000 cP
350000 - 550000 cP
Dynamic
Dow Corning 9045 Silicone Elastomer Blend
A mixture of high molecular weight silicone elastomers (dimethicone crosspolymer) in cyclopentasiloxane for use in skincare, suncare, shower gel, hair care, and color cosmetic applications.Informati..
Viscosity 350000 - 550000 cP

@Temperature 23.0 °C
350000 - 550000 cP

@Temperature 73.4 °F
0.5 rpm
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive
Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400..