Polymer Property : Viscosity = 600 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 600 - 900 cP
<br>@Temperature 25.0 °C
600 - 900 cP
<br>@Temperature 77.0 °F
Northstar Polymers PLA-012 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 600 cP
600 cP
Resinlab® RC8040 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Viscosity 600 - 1200 cP
<br>@Temperature 71.1 °C
600 - 1200 cP
<br>@Temperature 160 °F
Northstar Polymers PAA-109 Curing Agent
Information provided by Northstar Polymers.
Viscosity 600 - 4200 cP
<br>@Temperature 140 - 140 °C
600 - 4200 cP
<br>@Temperature 284 - 284 °F
Average value: 1.60e+6 cP Grade Count:6
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Viscosity 600 cP
<br>@Temperature 30.0 °C
600 cP
<br>@Temperature 86.0 °F
DSM Somos® 8110 Epoxy Photopolymer &nbsp;(discontinued **)
DescriptionDSM Somos® 8110 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and ..
Viscosity 600 - 1000 cP
600 - 1000 cP
Huntsman AroCy XU 378 Cyanate Ester
Comments/Applications: Novolac cyanate ester. High temperature composites and adhesives, where a Tg greater than 300°C is required.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemic..
Viscosity 600 - 1800 cP
600 - 1800 cP
Huntsman Araldite GZ 488 N-40 US Bisphenol A Epoxy Solution
Weight per Epoxide (EEW, g/eq) 3570 to 5500. Max color is 5.Comments/Applications: Very high molecular weight solid epoxy (8,000 - 10,000), 40% solids in MEK. Outstanding adhesion, excellent flexi..
Viscosity 600 - 1000 cP
600 - 1000 cP
25% Toluene Solution at 25°C; BAM 922
Kraton® D1114 P (SIS) Linear Triblock Copolymer
Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: ..
Viscosity 600 cP
<br>@Temperature 23.0 °C
600 cP
<br>@Temperature 73.4 °F
Master Bond EP19HT One Component, Storage Stable Epoxy System
Master Bond Polymer System EP19HT is a storage stable one component liquid epoxy resin system for durable, high performance adhesive/sealants, impregnants and liners. It features excellent storage c..
Viscosity 600 - 2300 cP
600 - 2300 cP
Milled Cement; Zeon Test #327
Zeon Chemicals Nipol® 1000x88 Nitrile Elastomer
Nipol 1000X88 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient antioxidant is added during manufacture for normal storage conditions.Excellent in adhesives whe..
Viscosity 600 cP
600 cP
Loctite® 4471 Surface Insensitive Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Viscosity 600 cP
600 cP
Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant
Excellent adhesion to metals, plastics, ceramics and glass. High bond strength, low moisture absorption, high thermal stability, low shrinkage and excellent chemical, electrical, and radiation resi..
Viscosity 600 cP
<br>@Temperature 180 °C
600 cP
<br>@Temperature 356 °F
Melt; ETM 22-31
ExxonMobil ESCOREZ™ 5415 Petroleum Hydrocarbon Resin
Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly..
Viscosity 600 cP
<br>@Temperature 25.0 °C
600 cP
<br>@Temperature 77.0 °F
Esstech X-738-0000 Ethoxylated Bis Phenol A Dimethacrylate, C83H144O34
This form of EBPADMA has 30 units of ethoxylation. It has a high degree of conversion neat and when blended with bisGMA. It also offers high levels of water absorption. Listed on the Toxic Substanc..
Viscosity 600 cP
<br>@Temperature 50.0 °C
600 cP
<br>@Temperature 122 °F
Cytec EN-2555 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Viscosity 600 cP
600 cP
25% toluene solution; MA 04-3-064
Dynasol Calprene® 540 Thermoplastic Rubber SBS Dry
Calprene 540 is a 60/40 Butadiene/Styrene thermoplastic copolymer, polymerized in solution and having a linear structure. This product is presented in pellet form and has excellent optical propertie..
Viscosity 600 cP
600 cP
B Side
ACC EP EF EPI Engineered Polymers Extra Flex Polyurea
EP EF, Extra Flex Polyurea, “Powered by Reactamine® Technology, is a two component 100% solid Polyurea, with superior performance in industrial applications. EP EF displays extremely fast cure tim..
Viscosity 600 cP
600 cP
B Side
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer
EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria..
Viscosity 600 cP
600 cP
Uncatalyst QM 100
ACC QM 100 QSI Quantum Silicones Clear 30 Durometer Condensation Cure Material
QM 100 is a two component, room temperature condensation cure silicone material. The cured rubber is a crystal clear material designed specifically for the special effects market. The materials' cla..
Viscosity 600 - 900 cP
600 - 900 cP
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Gray-ceramic inorganic coating to 1400°F.
Viscosity 600 - 900 cP
600 - 900 cP
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. White-ceramic inorganic coating to 1500°F.
Viscosity 600 cP
600 cP
uncured
Atom Adhesives AA-BOND FS227 Epoxy Adhesive
AA-BOND FS227 is a thixotropic polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wetting, toughness, a..
Viscosity 600 - 800 cP
600 - 800 cP
Aremco Pyro-Paint™ 634-AS High Temperature Refractory Coating
This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting ..
Viscosity 600 cP
600 cP
Abatron AboCast 8103-13 One-Component Epoxy
AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested..
Viscosity 600 cP
600 cP
BASF Pluronic® 17 R4 Block Copolymer Surfactant
Description: Pluronic 17R4 is a difunctional block copolymer surfactant with terminal secondary hydroxyl groups. A nonionic surfactant that is 100% active and relatively non-toxic.Information provi..
Viscosity 600 cP
600 cP
B Side
ACC EP RSP EPI Engineered Polymers Silicone Polyurea
EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time..
Viscosity 600 cP
600 cP
Von Roll Isola IMI Varnish 73527 Solventless Polyester Varnish for Electrical Insulation
Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usa..
Viscosity 600 cP
600 cP
Mixed
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System
Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru..
Viscosity 600 cP
600 cP
Solvay ANTAROX® 17-R-4 Surfactant
Chemical Name: EO/PO BLOCK COPOLYMERCAS: 9003-11-6, 7732-18-5Water solubility: SolubleAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: ANTAROX 17-R-4 is dispersible i..
Viscosity 600 - 1000 cP
600 - 1000 cP
#3 SP @ 60 rpm; RP-0596
Solvay RHODOLINE® 643 Surfactant
Description :Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer..