| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | |
|
ND Industries High Temperature SuperGlue 311
Very high viscosity with thermal cycling resistance
|
|||
| Viscosity | 0.0400 - 6000 cP | 0.0400 - 6000 cP | Average value: 1190 cP Grade Count:51 |
|
Overview of materials for Styrene/Butadiene/Styrene (SBS)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o..
|
|||
| Viscosity | 3000 - 6000 cP | 3000 - 6000 cP | |
|
Huntsman HY 840 US Polyamide
Approx. H+ equivalent weight 130. Mix Ratio with GY 6010 is 81.Comments/Applications: Solvent free, low viscosity, high amine content with higher flexibility and toughness. Flexible mix ratio 33 ..
|
|||
| Viscosity |
3000
-
6000
cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
3000
-
6000
cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2110414D7 UV Silver Flexographic Ink
UV curable Silver conductor ink specifically designed for printing on to polymeric substrates using flexographic printing. Ink can be printed at speeds up to 13m/min, with good line definition and ..
|
|||
| Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 30% solid in Anone |
|
Taiwan Sheen Soon Sheenthane® A7710 TPU for Ink
Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen..
|
|||
| Viscosity | 1000 - 6000 cP | 1000 - 6000 cP | LVT SP #3, 12 rpm; RP-17619 |
|
Solvay MIRACARE® SLB-205/N Surfactant
Description: Miracare SLB-205/N is a free flowing, high active surfactant concentrate used in the preparation of structured liquids. It is a surfactant base used to stabilize additives applied in a ..
|
|||
| Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | Part B |
|
Master Bond EP21ARHT Two component epoxy adhesive, sealant, coating and encapsulating system
Product Description: Master Bond EP21ARHT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a convenient 100 to 50 mix ratio by weight an..
|
|||
| Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | |
|
Master Bond EP46HT Epoxy Adhesive for Structural Bonding
Description: Master Bond System EP46HT is a newly formulated two component high performance heat resistant epoxy resin system with excellent mechanical strength and chemically resistant properties f..
|
|||
| Viscosity |
2400
-
6000
cP @Temperature 150 °C |
2400
-
6000
cP @Temperature 302 °F |
542-111 |
|
Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified
Product Description: Epolene C-18 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and ..
|
|||
| Viscosity |
2400
-
6000
cP @Temperature 150 °C |
2400
-
6000
cP @Temperature 302 °F |
542-111 |
|
Westlake Epolene® C-18P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-18P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and ..
|
|||
| Viscosity |
2400
-
6000
cP @Temperature 150 °C |
2400
-
6000
cP @Temperature 302 °F |
542-111 |
|
Westlake Epolene® C-19 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Product Description: Epolene C-19 is a branched low density polyethylene modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersion, and ..
|
|||
| Viscosity |
5000
-
6000
cP @Temperature 23.0 °C |
5000
-
6000
cP @Temperature 73.4 °F |
|
|
Master Bond EP34CA Low Viscosity Heat Resistant Epoxy System
Master Bond EP34CA is a low viscosity, polyfunctional, heat resistant epoxy resin designed for use in high performance composite structures, potting and casting applications. EP34CA can be used up t..
|
|||
| Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | Part B |
|
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System
Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings...
|
|||
| Viscosity | 1200 - 6000 cP | 1200 - 6000 cP | Thixotropic |
|
Loctite® 242 Medium Strength Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
|
|||
| Viscosity |
4000
-
6000
cP @Temperature 23.0 °C |
4000
-
6000
cP @Temperature 73.4 °F |
50 rpm |
|
Epoxy Technology EPO-TEK® 354 High Temperature Epoxy
Product Description: EPO-TEK® 354 is a two component, high Tg epoxy designed for semiconductor packaging in medical, fiber optic and optoelectronic assemblies. It is an electrically and thermally i..
|
|||
| Viscosity |
4000
-
6000
cP @Temperature 23.0 °C |
4000
-
6000
cP @Temperature 73.4 °F |
50 rpm |
|
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy
Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic..
|
|||
| Viscosity |
3500
-
6000
cP @Temperature 23.0 °C |
3500
-
6000
cP @Temperature 73.4 °F |
50 rpm |
|
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy
Material Description: A slightly longer pot life version of EPO-TEK®353ND designed for high temperature, optical and structural applications inside the semiconductor, hybrid, electronic, fiber opti..
|
|||
| Viscosity |
3500
-
6000
cP @Temperature 23.0 °C |
3500
-
6000
cP @Temperature 73.4 °F |
50 rpm |
|
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy
Product Description: EPO-TEK® H20E-HC is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al..
|
|||
| Viscosity |
3000
-
6000
cP @Temperature 23.0 °C |
3000
-
6000
cP @Temperature 73.4 °F |
50 rpm |
|
Epoxy Technology EPO-TEK® M10-D Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
|
|||
| Viscosity | 4500 - 6000 cP | 4500 - 6000 cP | |
|
Abatron AboCast/AboCure 8109-8
All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi..
|
|||
| Viscosity | 2000 - 6000 cP | 2000 - 6000 cP | |
|
3M Novec™ FC-4430 Fluorosurfactant
3M™ Novec™ Fluorosurfactant FC-4430 is a non-ionic polymeric fluorochemical surfactant belonging to a class of coating additives which provide low surface tensions in coating systems best served b..
|
|||
| Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 50-6 |
|
Abatron AboCast 50-6/AboCure 50-12 Epoxy
Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Colorless. Shelf life is 12+ months.
|
|||
| Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 50-6 |
|
Abatron AboCast 50-6/AboCure 50-17 Epoxy
Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Medium Amber color. Shelf life is 12+ months.
|
|||
| Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 50-6 |
|
Abatron AboCast 50-6/AboCure 50-1 Epoxy
Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months.
|
|||
| Viscosity |
4000
-
6000
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
4000
-
6000
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2060602D1 Membrane Touch Switch Paste
The ink should be gently stirred before use avoiding introduction of air bubbles. It is a polymer based system for printing on polyester, PVC, etc.Can be used in membrane touch switch applicationsSc..
|
|||
| Viscosity | 3000 - 6000 cP | 3000 - 6000 cP | |
|
3M Novec™ FC-4432 Fluorosurfactant
3M fluorosurfactant FC-4432 is a non-ionic polymeric fluorochemical surfactant that offers excellent wetting, leveling and flow control in a variety of waterborne, solvent-borne and high-solids orga..
|
|||
| Viscosity |
3500
-
6000
cP @Shear Rate 230 1/s, Temperature 25.0 °C |
3500
-
6000
cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
|
Gwent Electronic Materials C2010309P3 Platinum Paste
This product has been designed as a platinum paste suitable for high temperature firing applications on to electro-ceramic substrates such as NTC. It is capable of withstanding repeated firing at h..
|
|||