Polymer Property : Viscosity = 600000 cP Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Viscosity 600000 - 600000 cP

@Temperature 420 - 420 °C
600000 - 600000 cP

@Temperature 788 - 788 °F
Average value: 600000 cP Grade Count:1
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i..
Viscosity 350000 - 600000 cP

@Temperature 220 - 220 °C
350000 - 600000 cP

@Temperature 428 - 428 °F
Average value: 475000 cP Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Viscosity 200000 - 600000 cP
200000 - 600000 cP
Part A
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive
Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation ..
Viscosity 400000 - 600000 cP
400000 - 600000 cP
Part B
Master Bond EP33ND Epoxy Paste Resists Harsh Chemicals
Description: Master Bond EP33ND is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very g..