Physical Properties Metric English Comments
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PBA-052 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PBA-055 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PBA-058 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 - 1100 cP

@Temperature 25.0 °C
700 - 1100 cP

@Temperature 77.0 °F
Northstar Polymers PPA-019 Polyether Curing Agent
Information provided by Northstar Polymers.
Viscosity 700 cP
700 cP
Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Viscosity 700 cP

@Temperature 30.0 °C
700 cP

@Temperature 86.0 °F
DSM Somos® 7110 Epoxy Photopolymer, Green Parts  (discontinued **)
DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..
Viscosity 700 cP

@Temperature 30.0 °C
700 cP

@Temperature 86.0 °F
DSM Somos® 7120 Epoxy Photopolymer, Green Parts  (discontinued **)
DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u..
Viscosity 700 - 527068 cP

@Shear Rate 10.0 - 5000 1/s
700 - 527068 cP

@Shear Rate 10.0 - 5000 1/s
Average value: 221000 cP Grade Count:3
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Viscosity 700 - 1300 cP
700 - 1300 cP
Huntsman XB 4122 Multifunctional Resin
Weight per Epoxide (EEW, g/eq) 330 to 365. Max color is 5.Comments/Applications: Low viscosity, unmodified tough flexible epoxy with excellent workability. For use as a modifier in high solids coa..
Viscosity 700 - 1200 cP
700 - 1200 cP
Lucite International Colacryl ® TS1171/1 Acrylic Solution Resin
Butyl methacrylate-Methyl methacrylate copolymerThis product is a fairly soft and flexible copolymer with reasonable abrasion resistance. It has good UV resistance and is therefore suitable for outd..
Viscosity 700 cP
700 cP
Solution Viscosity; ASTM D455
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)
Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi..
Viscosity 700 cP

@Temperature 25.0 °C
700 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Bond 342-13ACC Single Component Low Viscosity Epoxy Adhesive
TRA-BOND 342-13ACC single component, low viscosity epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature in 24 hours ..
Viscosity 700 cP

@Temperature 23.0 °C
700 cP

@Temperature 73.4 °F
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy
Master Bond Polymer System EP29LPSP is a two component, high performance, modified low temperature heat cured epoxy system specially formulated for cryogenic applications. EP29LPSP is serviceable at..
Viscosity 700 - 1000 cP
700 - 1000 cP
NOV QC 020
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Viscosity 700 cP
700 cP
dynamic
Dow Corning BF 20 PLUS ANTIFOAM EMULSION
20% active silicone antifoam emulsion suitable for controlling foam in end-use applications of many liquid detergent products.Information provided by Dow Corning
Viscosity 700 cP
700 cP
dynamic
Dow Corning FLUOROGEL® 4-8022
One-part, translucent, heat cure, UV indicator, fuel and solvent resistant.Information provided by Dow Corning
Viscosity 700 cP
700 cP
Dow Corning SYL-OFF® 7138 HIGH SPEED CROSSLINKER
Syl-Off® 7138 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue, and Syl-Off® 7678 Cr..
Viscosity 700 cP
700 cP
Dynamic
Dow Corning SYL-OFF® PMCP7138 High Speed Crosslinker
Syl-Off® 7137 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue, and Syl-Off® 7678 Cr..
Viscosity 700 cP
700 cP
Dow PAPI™ 580 N Polymeric MDI
PAPI™ 580 N polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has high functionality (value of 3.0) and relatively high viscosity. Recommended for use in polyi..
Viscosity 700 cP
700 cP
BASF Lupranate® M70L Isocyanate
Description: Lupranate® M70L Isocyanate is a solvent-free, medium-viscosity polymethylene polyphenypolyisocyanate. Lupranate M70L Isocyanate, having a higher viscosity than Lupranate M20S, is parti..
Viscosity 700 - 1100 cP
700 - 1100 cP
Beijing Ranger Chem WSR615 Liquid Epoxy Resin
Information provided by Beijing Ranger Chemical Co.
Viscosity 700 cP
700 cP
BASF Lupranate® 259 Isocyanate
Description: Lupranate® 259 Isocyanate is a modified pure MDI. No 259 Isocyanate is applicable for use in all CASE applications.Information provided by BASF
Viscosity 700 cP
700 cP
BASF Lupranate® MP102 Isocyanate Modified MDI
Description: Lupranate® MP102 Isocyanate is a liquid, modified short chain prepolymer based on pure 4,4’-diphenylmethane diisocyanate (MDI). Lupranate MP102 Isocyanate is used in conjunction with ..
Viscosity 700 cP

@Temperature 25.0 °C
700 cP

@Temperature 77.0 °F
Uncured
Permabond HM135 Anaerobic Retainer
Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras..
Viscosity 700 cP

@Temperature 200 °C
700 cP

@Temperature 392 °F
Melt
Unitika elitel UE3500 Polyester, Flake
High molecular weight, High toughness, High strength, High elongationUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from produc..
Copyright © lookpolymers.com All Rights Reserved